Journal Articles
Alloy Digest (2009) 58 (9): SA-606.
Published: 01 September 2009
... ATI 500-MIL High Hard is a specialty steel of wrought Ni-Cr-Mo specialty steel for armor plate. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2009) 58 (10): SA-610.
Published: 01 October 2009
... cutting. Thermal cutting may produce some distortion, but is typically less than when thermally cutting liquid quenched materials. Product Forms Available: ATI 500-MIL specialty steel is available in standard mill plate gages or 4.762 15.9 mm (0.1875 0.625 in Inquire for other gages. Applications: Armor...
Journal Articles
Alloy Digest (2013) 62 (7): SS-1150.
Published: 01 July 2013
... ( circular-mil/ft) 0.587 (353) Mechanical Properties: (Typical annealed tensile properties) Yield strength, MPa (ksi) 310 (45.0) Tensile strength, MPa (ksi) 496 (72.0) Elongation, 51 mm (2 in % 31.0 Hardness, RB 82.0 Elevated temperature tensile properties are shown in Table 1 and compared there to ATI 409...
Journal Articles
Alloy Digest (2020) 69 (10): SS-1328.
Published: 01 October 2020
... capacity J/(kg K) (cal/(g °C)) 0 100 °C (32 212 °F) 502 (0.120) Electrical resistivity m circular-mil/ft) 20 °C (68 °F) 0.94 (565) Magnetic permeability(a) H/m 1.02 For solution annealed condition. (a) At 200 Oe (15.9 kA/m) Mechanical Properties See Tables 1 and 2. Corrosion Resistance ATI 310S has...
Journal Articles
Alloy Digest (2021) 70 (10): Ni-776.
Published: 01 October 2021
...) (0.298)(a) Thermal 20 200 °C conductivity W/(m K) (68 392 °F) 13.2 Specific heat (Btu/(h·ft·°F)) 20 300 °C (7.33)(b) capacity (68 572 °F) Electrical J/(kg K) 20 400 °C 13.5 resistivity (cal/(g °C)) (68 752 °F) (7.5)(b) 20 500 °C m (68 932 °F) 13.7 circular-mil/ft) (7.61)(b) 20 °C (68 °F) 13.9 20 °C (7.72...
Journal Articles
Alloy Digest (2021) 70 (4): SS-1333.
Published: 01 April 2021
... 29 18.7 20 °C (10.8) 359 52 172 25 (68 °F) 500 241 35 148 22 (0.12) Specific heat J/(kg K) 145 21 120 18 capacity (cal/(g °C)) 0.78 Electrical (469) 72 11 resistivity m circular-mil/ 1.02 max(b) Typical values. (a) Gauge length = 50 mm (2 in.) Magnetic permeability(a) ft) Table 3 Modulus...
Journal Articles
Alloy Digest (2021) 70 (5): SS-1334.
Published: 01 May 2021
... Specific heat (cal/(g °C)) (32 1000 °F) (9.3) 649 1200 37 capacity 760 1400 517 75 238 35 39 Electrical m 0 649 °C 17.3 871 1600 50 resistivity circular-mil/ft) (32 1200 °F) (9.6) 982 1800 490 71 221 32 Magnetic permeability(a) H/m 100 °C 18.0 441 64 200 29 (212 °F) (10.0) 500 °C 359 52 172 25 (932 °F...
Journal Articles
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
... ( 130) 779 (113) 1069 (155) 57 70 ( 94) 710 (103) 965 (140) 61 50 ( 58) 662 (96) 889 (129) 67 20 ( 4) 614 (89) 820 (119) 54 21 (70) 524 (76) 738 (107) 41 93 (200) 455 (66) 655 (95) 32 149 (300) 427 (62) 607 (88) 27 204 (400) 386 (56) 600 (87) 26 260 (500) 386 (56) 586 (85) 22 Fig. 1 ATI 2003 LDSS...
Journal Articles
Alloy Digest (2020) 69 (5): SS-1318.
Published: 01 May 2020
... 12.0 15.0 Iron bal (a) Maximum values unless indicated otherwise. Source: ATI and ASTM A240/ A240M:2019 Physical Properties Property Unit At Value Density kg/m3 (lb/in.3) 8030 (0.29) Coefficient of linear thermal expansion 10 6/K (10 6/°F) 20 100 °C (68 212 °F) 15.7 (8.7) 20 500 °C (68 932 °F) 17.6...
Journal Articles
Alloy Digest (2020) 69 (12): Ti-173.
Published: 01 December 2020
...(a) (1825±25) Density kg/m3 (lb/in.3) RT 4420 (0.160) Coefficient of linear thermal expansion 10 6/K (10 6/°F) 20 100 °C (68 212 °F) 9.0 (5.0) Thermal conductivity W/(m K) (Btu/(h·ft·°F)) RT 6.6 (3.8) Specific heat capacity J/(kg K) (cal/(g °C)) RT 526 (0.126) Electrical resistivity m circular-mil/ft) RT...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-595.
Published: 01 December 2002
... Nickelvac K-500 is a nickel-copper alloy with age-hardening properties imparted by alloying additions of aluminum and titanium. The alloy is characterized by excellent corrosion resistance in an extensive range of natural and chemical environments, excellent resistance to chloride-ion stress...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... (lb/in.3 ) 8327 (0.302) Electrical resistivity, 20 °C (68 °F), 1.22 (734) µ m ( circular-mil/ft) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 20 100 °C (68 212 °F) 12.0 (6.7) 20 200 °C (68 392 °F) 12.4 (6.9) 20 400 °C (68 752 °F) 13.0 (7.2) 20 600 °C (68 1110 °F) 13.9 (7.7) 20 800 °C...
Journal Articles
Alloy Digest (2004) 53 (8): SS-906.
Published: 01 August 2004
... Properties: Density at 20 °C (68 °F), 8000 (0.29) kg/m3 (lb/in.3 ) Resistivity at 20 °C (68 °F), µ m 0.92 (550) ( circular-mil/ft) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 20 100 °C (68 212 °F) 15.0 (8.3) 20 300 °C (68 572 °F) 16.5 (9.2) 20 500 °C (68 932 °F) 17.3 (9.6) Thermal...
Journal Articles
Alloy Digest (2000) 49 (2): SS-776.
Published: 01 February 2000
... 6/K (10 6/°F) 20 100 C (68 212 °F) 16.6 (9.2) 20-500 C (32-932 °F) 18.2 (10.1) Structure Austenite Melting range, C ( F) 1393 1443 (2540 2630) Electrical resistivity at 21 C (70 F), m ( circular-mil/ft) 0.73 (439) Mechanical Properties: Modulus of elasticity, GPa (10 6 psi) 193 207 (28 30...
Journal Articles
Alloy Digest (1982) 31 (7): Cu-440.
Published: 01 July 1982
... ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engineering Publications, Inc. AtI rights reserved. ISSN:OOZ-614X Pubhhed by Xg&wZg=& hJ- Upper Montchir, New Jersey MUELLER COPPER 1470 (Sulfur-Bearing High-Conductivity Copper) MUELLER COPPER 1470 is a high-conductivity copper to which sulfur has been...
Journal Articles
Alloy Digest (2006) 55 (4): SS-958.
Published: 01 April 2006
... (0.275) (lb/in.3 ) Thermal conductivity, room temperature, 19.2 (11.1) W/m . K (Btu/(ft . h . °F)) Resistivity, room temperature, 0.733 (441) . m ( circular-mil/ft) Coefficient of linear thermal expansion, push-rod dilatometer, 10-6/K (10-6/°F) 20 100 °C (68 212 °F) 10.2 (5.7) 20 260 °C (68 500 °F...
Journal Articles
Alloy Digest (2001) 50 (9): SS-829.
Published: 01 September 2001
..., 20 ° C (68 ° F), m 0.63 (379) ( circular-mil/ft) Specific heat capacity, at 0 100 ° C (32 212° F), 460 (0.11) J/kg K (Btu/lb ° F) Thermal conductivity, at 20 100 ° C (68 212° F), 24.2 (14.0) W/m K (Btu/(ft h ° F)) Coefficient of linear thermal expansion, 10 6/K (10 6/° F) 20 100 ° C...