Skip Nav Destination
Close Modal
Search Results for
ATI 50 Alloy
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 80 Search Results for
ATI 50 Alloy
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (10): SS-1103.
Published: 01 October 2011
... ATI 50 Alloy is an austenitic stainless steel strengthened with nitrogen. It is superior to AISI Type 316L in both strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion...
Abstract
View article
PDF
ATI 50 Alloy is an austenitic stainless steel strengthened with nitrogen. It is superior to AISI Type 316L in both strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1103. Producer or source: ATI Allegheny Ludlum Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (6): SS-1348.
Published: 01 June 2022
... deformation, the alloy hardens solely through the mechanism of lattice strain hardening. The alloy is not hardenable by heat treatment. Cold working is the only method for increasing the strength of ATI 219. Table 2 Magnetic permeability at room temperature Percent cold reduction 0 10 30 50 65 Magnetic...
Abstract
View article
PDF
ATI 219, also known by the more familiar 21-6-9 or XM-11 designations, is a nitrogen-bearing austenitic stainless steel that has substantially higher strength than the standard austenitic stainless steels. The alloy remains non-magnetic even after substantial cold forming and exposure to subzero temperatures. Many of the applications for ATI 219 make use of its combination of high strength and nonmagnetic properties, even at very low temperatures. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1348. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (9): SA-606.
Published: 01 September 2009
... Exceeds spec 8 0.315 .50 cal AP 570.9 1873 Exceeds spec 9.52 0.375 .50 cal AP 631.9 2073 Exceeds spec 12.7 0.5 .50 cal AP 743.7 2440 Exceeds spec 15.87 0.625 14.5mmB32 740.1 2428 Exceeds spec 19.05 0.75 14.5mmB32 816.6 2679 Exceeds spec 25.4 1 14.7mmBS41 860.1 2822 Exceeds spec ATI 500-MIL plate...
Abstract
View article
PDF
ATI 500-MIL High Hard is a specialty steel of wrought Ni-Cr-Mo specialty steel for armor plate. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-606. Producer or source: ATI Defense.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (3): SS-1139.
Published: 01 March 2013
...) 341 (49.4) 18 649 (1200) 138 (20.0) 248 (36.0) 30 760 (1400) 56.5 (8.2) 138 (20.0) 35 871 (1600) 33.1 (4.8) 40.7 (5.9) 50 DOI: 10.31399/asm.ad.ss1139 metal arc processes. Properly welded, the ATI 436S alloy retains corrosion resistance and most of the mechanical properties of the base metal...
Abstract
View article
PDF
ATI 436S is a ferritic stainless steel stabilized with titanium. It is superior to ATI Type 409 and 430 in general and pitting corrosion resistance. The ATI 436S alloy exhibits machining, welding, and forming characteristics similar to those of other stabilized, ferritic stainless steels. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1139. Producer or source: Allegheny Ludlum.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (5): Ti-166.
Published: 01 May 2020
... ATI 3-2.5 is a Titanium-3Aluminum-2.5Vanadium alloy that has higher strength than unalloyed titanium and is much more amenable to cold working than Ti-6Al-4V. This near-alpha, alpha-beta alloy is generally used in the annealed or cold-worked and stress-relieved conditions. This datasheet provides...
Abstract
View article
PDF
ATI 3-2.5 is a Titanium-3Aluminum-2.5Vanadium alloy that has higher strength than unalloyed titanium and is much more amenable to cold working than Ti-6Al-4V. This near-alpha, alpha-beta alloy is generally used in the annealed or cold-worked and stress-relieved conditions. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-166. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (1): Ti-149.
Published: 01 January 2012
... ATI Ti-5Al-2Sn-2Zr-4Cr-4Mo is known as Ti-17 alloy and is a beta-rich material for large aerospace components. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Abstract
View article
PDF
ATI Ti-5Al-2Sn-2Zr-4Cr-4Mo is known as Ti-17 alloy and is a beta-rich material for large aerospace components. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-149. Producer or source: ATI Allvac.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (3): Ti-158.
Published: 01 March 2017
... ATI 6-2-4-2 alloy is a near-alpha high strength titanium alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-158. Producer or source...
Abstract
View article
PDF
ATI 6-2-4-2 alloy is a near-alpha high strength titanium alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-158. Producer or source: Allegheny Technologies Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
... ATI 2003 lean duplex stainless steel (LDSS) is a molybdenum-enhanced, duplex stainless steel alloy. Cr, Ni, Mo, and N are controlled to give a phase balance similar to that of ATI 2205 duplex stainless steel, while reducing costs. This datasheet provides information on composition, physical...
Abstract
View article
PDF
ATI 2003 lean duplex stainless steel (LDSS) is a molybdenum-enhanced, duplex stainless steel alloy. Cr, Ni, Mo, and N are controlled to give a phase balance similar to that of ATI 2205 duplex stainless steel, while reducing costs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1258. Producer or source: Allegheny Technologies Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (8): Ti-169.
Published: 01 August 2020
... ATI 6-2-4-2 is a near-alpha, high strength, titanium alloy that exhibits a good combination of tensile strength, creep strength, toughness, and long-term stability at temperatures up to 425 °C (800 °F). Silicon up to 0.1% frequently is added to improve the creep resistance of the alloy...
Abstract
View article
PDF
ATI 6-2-4-2 is a near-alpha, high strength, titanium alloy that exhibits a good combination of tensile strength, creep strength, toughness, and long-term stability at temperatures up to 425 °C (800 °F). Silicon up to 0.1% frequently is added to improve the creep resistance of the alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ti-169. Producer or Source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (5): SS-1035.
Published: 01 May 2009
... ATI S240 alloy is a high-strength precipitation-hardening alloy with advantages in simple thermal mechanical processing, corrosion resistance, and lower costs than similar-strength alloys. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Abstract
View article
PDF
ATI S240 alloy is a high-strength precipitation-hardening alloy with advantages in simple thermal mechanical processing, corrosion resistance, and lower costs than similar-strength alloys. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-1035. Producer or source: ATI Allvac.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (6): Ti-150.
Published: 01 June 2013
.... It was developed by General Electric for fan and compressor discs. ATI 17 Ti-5Al-2Sn-2Zr-4Cr-4Mo (Beta Rich Titanium Alloy) ATI 17 Ti-5Al- 2Sn-2Zr-4Cr-4Mo Chemical Composition, wt Aluminum 4.5 5.5 Tin 1.5 2.5 Chromium 3.5 4.5 Molybdenum 3.5 4.5 Zirconium 1.5 2.5 Iron 0.3 max Oxygen 0.08 0.13 Nitrogen 0.04 max...
Abstract
View article
PDF
ATI 17 Ti-5Al-2Sn-2Zr-4Cr-4Mo is also known as Ti-17. It was developed by General Electric for fan and compressor discs. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-150. Producer or source: Allvac, An Allegheny Technologies Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (4): SS-1244.
Published: 01 April 2016
... are shown in Fig. 2. Whereas corrosion was evident on the ATI 409 alloy sample after the first cycle, the ATI 436S alloy does not show any significant weight loss until the samples have experienced more than 50 oxidation/corrosion cycles. The higher chromium of the ATI 436S alloy provides better oxidation...
Abstract
View article
PDF
ATI 436S ferritic stainless is a single phase alloy in the same family as Type 409 and is common to many of those properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1244. Producer or source: Allegheny Ludlum.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Co-133.
Published: 01 February 2021
... ATI 35N is a wrought, multi-phase Co-Ni-Cr-Mo alloy that can be heat treated to achieve very high strength, while maintaining excellent toughness, ductility, and corrosion resistance. To achieve tensile strength levels of 1795 to 2070 MPa (260 to 300 ksi), the alloy is cold worked...
Abstract
View article
PDF
ATI 35N is a wrought, multi-phase Co-Ni-Cr-Mo alloy that can be heat treated to achieve very high strength, while maintaining excellent toughness, ductility, and corrosion resistance. To achieve tensile strength levels of 1795 to 2070 MPa (260 to 300 ksi), the alloy is cold worked and then precipitation hardened. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-133. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (9): Ti-182.
Published: 01 September 2021
... ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion...
Abstract
View article
PDF
ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or in storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-182. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (7): Ni-761.
Published: 01 July 2020
... ATI 75 (UNS N06075) is a nickel-chromium alloy with controlled additions of titanium and carbon; it derives its high temperature strength essentially from solid solution strengthening. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Abstract
View article
PDF
ATI 75 (UNS N06075) is a nickel-chromium alloy with controlled additions of titanium and carbon; it derives its high temperature strength essentially from solid solution strengthening. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: Ni-761. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (2): Ni-756.
Published: 01 February 2020
... ATI 10242 is an age-hardenable nickel-molybdenum-chromium alloy that derives its strength from a long-range ordering reaction during aging. This ordering reaction not only provides the alloy’s strength, but also imparts excellent thermal stability. This datasheet provides information...
Abstract
View article
PDF
ATI 10242 is an age-hardenable nickel-molybdenum-chromium alloy that derives its strength from a long-range ordering reaction during aging. This ordering reaction not only provides the alloy’s strength, but also imparts excellent thermal stability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as forming, machining, and joining. Filing Code: Ni-756. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (12): Ni-765.
Published: 01 December 2020
... ATI 6230 is a solid-solution strengthened, corrosion and heat-resistant, Ni-Cr-W-Mo-Al-La alloy. It is typically used for parts requiring good resistance to oxidizing environments up to 1150 °C (2100 °F) and relatively high strength up to 980 °C (1800 °F); however, usage is not limited...
Abstract
View article
PDF
ATI 6230 is a solid-solution strengthened, corrosion and heat-resistant, Ni-Cr-W-Mo-Al-La alloy. It is typically used for parts requiring good resistance to oxidizing environments up to 1150 °C (2100 °F) and relatively high strength up to 980 °C (1800 °F); however, usage is not limited to such applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-765. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (9): SS-1157.
Published: 01 September 2013
... and corrosion resistance as well as forming. Filing Code: SS-1157. Producer or source: Allegheny Ludlum. Producer or Source: Allegheny Ludlum Copyright © ASM International® 2013 2013 ASM International ATI 441 HP chemical composition corrosion-resistant alloys high-temperature alloys oxidation...
Abstract
View article
PDF
ATI 441 HP is a ferritic stainless steel with good oxidation and corrosion resistance. It was developed for severe tube bending and forming. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming. Filing Code: SS-1157. Producer or source: Allegheny Ludlum.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (12): SS-1109.
Published: 01 December 2011
... ATI 2304 is a lean duplex alloy with a microstructure that consists of a nearly equal mixture of ferrite and austenite. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high...
Abstract
View article
PDF
ATI 2304 is a lean duplex alloy with a microstructure that consists of a nearly equal mixture of ferrite and austenite. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1109. Producer or source: Allegheny Technologies Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... ATI CP Grade 7 Titanium is an unalloyed titanium grade that contains 0.12–0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 7 Titanium is used in applications requiring excellent corrosion...
Abstract
View article
PDF
ATI CP Grade 7 Titanium is an unalloyed titanium grade that contains 0.12–0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 7 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, tensile properties and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-175. Producer or source: ATI.