Alloy Digest (2012) 61 (12): SS-1130.
Published: 01 December 2012
... ATI 412 alloy is a corrosion-resistant, dual-phase, 12% Cr stainless steel that offers a good combination of strength, ductility, toughness, wear resistance, and weldability. This alloy offers potential cost savings compared to less corrosion- and wear-resistant materials based on its longer...
Journal Articles
Alloy Digest (2011) 60 (12): SS-1109.
Published: 01 December 2011
... ATI 2304 is a lean duplex alloy with a microstructure that consists of a nearly equal mixture of ferrite and austenite. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (2013) 62 (11): Fe-162.
Published: 01 November 2013
..., housings for magnets, and transformer wedges. ATI 9 is a trademark of ATI Properties, Inc. DOI: 10.31399/asm.ad.fe0162 Producer: Allegheny Ludlum An Allegheny Technologies Company Pittsburgh, PA 1522-5479, USA www.ATImetals.com Tel: (412) 394-2800 ISSN: 002-614X FE-162B ...
Journal Articles
Alloy Digest (2016) 65 (3): Co-126.
Published: 01 March 2016
... ATI L-605 alloy is a high-temperature cobalt alloy with oxidation resistance to 1093 deg C (2000 deg F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming and heat...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... ATI 6-4 ELI, also known as Grade 23, is a higher purity grade of ATI Ti-6Al-4V for use in surgical and medical applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (2016) 65 (2): Co-125.
Published: 01 February 2016
... ATI 188 Alloy is a high temperature cobalt alloy with oxidation resistance to 1093 deg C (2000 deg F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming and heat treating...
Journal Articles
Alloy Digest (2017) 66 (3): Ti-158.
Published: 01 March 2017
..., extrusions, and wire. Applications: ATI 6-2-4-2 alloy is used in gas turbine engines for compressor blades, discs, and impellers. It also has applications in afterburner structures as well as for airframe skin applications. Producer: Allegheny Technologies Incorporated Pittsburgh, PA 15222, USA Tel: (412...
Journal Articles
Alloy Digest (2013) 62 (9): SS-1157.
Published: 01 September 2013
... ATI 441 HP is a ferritic stainless steel with good oxidation and corrosion resistance. It was developed for severe tube bending and forming. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (2016) 65 (4): SS-1244.
Published: 01 April 2016
... automotive and other exhaust systems. Producer: Allegheny Ludlum An Allegheny Technologies Company Pittsburgh, PA 15222, USA Tel: (412) 394-2800 www.ATImetals.com ISSN: 002-614X SS-1244B Formability: Formability of this alloy is similar to that of other ferritic stainless steels such as ATI 409 and ATI 439...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1131.
Published: 01 January 2013
... ATI 444 is a low-carbon and low-nitrogen ferritic stainless steel with 18Cr and 2Mo and is often referred to as "18-2". This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2015) 64 (8): SS-1222.
Published: 01 August 2015
... ATI 304B7 P/M is a borated austenitic stainless steel of the type 304 base. Boron addition is accomplished through powder metallurgy. The uniform, fine dispersion of boron containing particles resulting from the P/M process imparts superior neutron absorption and enhanced toughness and ductility...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1139.
Published: 01 March 2013
... 15222-5479, USA Tel: (412) 394-2800 www.ATImetals.com ISSN: 002-614X SS-1139B Table 2 100-hour oxidation in still air weight gain, mg/cm2 Temperature, °C (°F) ATI 409 ATI 436S 760 (1400) 0.167 0.193 816 (1500) 0.372 0.243 871 (1600) 3.45 0.424 927 (1700) 88.95 0.58 982 (1800) 0.836 1038 (1900...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1227.
Published: 01 October 2015
... ATI 316LN stainless is a low carbon, nitrogen-enhanced version of Type 316 stainless steel. This version is more intergranular and pitting resistant than Type 316. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
... ATI 2003 lean duplex stainless steel (LDSS) is a molybdenum-enhanced, duplex stainless steel alloy. Cr, Ni, Mo, and N are controlled to give a phase balance similar to that of ATI 2205 duplex stainless steel, while reducing costs. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2015) 64 (5): SS-1207.
Published: 01 May 2015
... Pittsburgh, PA 15222, USA Tel: (412( 394-2800 www.ATImetals.com ISSN: 002-614X SS-1207B Fig. 2 Critical crevice corrosion temperature of ATI 2102 LDSS comparison ...
Journal Articles
Alloy Digest (2013) 62 (7): SS-1150.
Published: 01 July 2013
... ATI 441 is a low-carbon and low-nitrogen ferritic stainless steel with 18 Cr and columbium. The alloy is typically used for exhaust system components. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (2013) 62 (10): SS-1158.
Published: 01 October 2013
...: (412) 394-2800 www.ATImetals.com Table 1 General corrosion in dilute reducing acids Boiling solution Corrosion rate, mm per year (in./y)(a) ATI 332Mo 625Alloy Type 316 10% sulfuric acid (base metal) 0.033 (0.0013) 0.64 (0.025) 16.2 (0.64) 10% sulfuric acid (weld metal) 0.031 (0.0012) 16.7 (0.66) 1...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1135.
Published: 01 February 2013
... alloys are available as sheet, strip, and plate product forms from Allegheny Ludlum. Tube or pipe products using ATI 409HP alloy are available from tube/pipe manufacturers. Producer: Allegheny Technologies Incorporated Pittsburgh, PA 15222-5479 USA Tel: (412) 394-2800 www.atimetals.com ISSN: 002-614X SS...
Journal Articles
Alloy Digest (2001) 50 (9): SS-829.
Published: 01 September 2001
... AL 439HP, AL 409HP, and AL 441HP are trademarks of ATI Properties, Inc. Fig. 1 Cyclic exhaust system condensate corrosion DOI: 10.31399/asm.ad.ss0829 runners where bend radii are often less than 2D. The AL 409HP, AL 439HP, and AL 441HP ferritic stainless steels have been developed specifically...
Journal Articles
Alloy Digest (2007) 56 (2): SA-560.
Published: 01 February 2007
... configuration. It may also be supplied as heat treated parts cut to the final configuration. K12 is trademark of ATI Properties, Inc. Fabricability: K12 plate is difficult to machine, flatten, or drill after heat treatment. As much as possible, such operations should be performed at least as a roughing...