1-1 of 1 Search Results for

ATI 316LN

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2015) 64 (10): SS-1227.
Published: 01 October 2015
... ATI 316LN stainless is a low carbon, nitrogen-enhanced version of Type 316 stainless steel. This version is more intergranular and pitting resistant than Type 316. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...