Skip Nav Destination
Close Modal
Search Results for
ATI 2003
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-14 of 14 Search Results for
ATI 2003
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2021) 70 (5): SS-1335.
Published: 01 May 2021
... ATI 2003 (UNS S32003) is a molybdenum-enhanced lean duplex stainless steel (LDSS) that was developed to fill the performance gap between type 316L (UNS S31603) and 2205 duplex (UNS S32205) stainless steels. ATI 2003 has reduced alloy content, which makes it less costly than 2205 duplex, yet ATI...
Abstract
View article
PDF
ATI 2003 (UNS S32003) is a molybdenum-enhanced lean duplex stainless steel (LDSS) that was developed to fill the performance gap between type 316L (UNS S31603) and 2205 duplex (UNS S32205) stainless steels. ATI 2003 has reduced alloy content, which makes it less costly than 2205 duplex, yet ATI 2003 retains the high strength level characteristic of duplex grades. Compared to type 316L, ATI 2003 has increased strength, better corrosion resistance, and greater cost stability. These and other factors make ATI 2003 an attractive alternative for a variety of applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1335. Producer or source: ATI.
Journal Articles
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
... ATI 2003 lean duplex stainless steel (LDSS) is a molybdenum-enhanced, duplex stainless steel alloy. Cr, Ni, Mo, and N are controlled to give a phase balance similar to that of ATI 2205 duplex stainless steel, while reducing costs. This datasheet provides information on composition, physical...
Abstract
View article
PDF
ATI 2003 lean duplex stainless steel (LDSS) is a molybdenum-enhanced, duplex stainless steel alloy. Cr, Ni, Mo, and N are controlled to give a phase balance similar to that of ATI 2205 duplex stainless steel, while reducing costs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1258. Producer or source: Allegheny Technologies Inc..
Journal Articles
Alloy Digest (2011) 60 (12): SS-1109.
Published: 01 December 2011
... are also shown for comparison. Figure 1 shows the ASME Section VIII Division 1 maximum allowable stress levels for ATI 2304 plate material. The maximum allowable stress levels for ATI 2003 LDSS and Type 316L are shown for comparison. Low-Temperature Impact Properties. Duplex stainless steels, such as ATI...
Abstract
View article
PDF
ATI 2304 is a lean duplex alloy with a microstructure that consists of a nearly equal mixture of ferrite and austenite. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1109. Producer or source: Allegheny Technologies Inc..
Journal Articles
Alloy Digest (2015) 64 (5): SS-1207.
Published: 01 May 2015
... tested, and both developed stress corrosion cracks in less than 1000 hours. The results of these tests are shown below. Type 304 Failed (850 hours) Type 316 Failed (530 940 hours) ATI 2012 Passed (1000 hours) ATI 2003 Passed (1000 hours) ATI 2205 Passed (1000 hours) Pitting and Crevice Corrosion...
Abstract
View article
PDF
ATI 2102 is a lean austenitic/ferritic duplex stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1207. Producer or source: Allegheny Ludlum.
Journal Articles
Alloy Digest (2003) 52 (2): Ni-601.
Published: 01 February 2003
... (N08825), but with the age-hardening constituents of titanium and aluminum to achieve high strength while maintaining excellent corrosion resistance. Allvac and Nickelvac are registered trademarks of ATI Properties, Inc. Fig. 1 Thermal conductivity Fig. 2 Coefficient of thermal expansion DOI: 10.31399...
Abstract
View article
PDF
Nickelvac 925 is an alloy similar to alloy 825 (N08825), but with the age-hardening constituents of titanium and aluminum to achieve high strength while maintaining excellent corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-601. Producer or source: Allvac Metals Company.
Journal Articles
Alloy Digest (2002) 51 (12): SS-869.
Published: 01 December 2002
... nickel and molybdenum alloy than the duplex stainless steel AL 2205, but is similar in both phase balance and mechanical properties. Applications include areas where resistance to both general and chloride-ion stress-corrosion crack- ing is important. AL 2003 and AL 2205 are trademarks of ATI Properties...
Abstract
View article
PDF
The AL 2003 alloy is a nitrogen-enhanced leaner nickel and molybdenum alloy than the duplex stainless steel AL 2205, but is similar in both phase balance and mechanical properties. Applications include areas where resistance to both general and chloride-ion stress-corrosion cracking is important. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-869. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (2003) 52 (10): Zr-11.
Published: 01 October 2003
.... Producer or source: ATI Wah Chang, Allegheny Technologies. Producer or Source: ATI Wah Chang, Allegheny Technologies Copyright © ASM International® 2003 2003 ASM International ASTM B 752 GRADE 702C cast zirconium alloys chemical composition corrosion-resistant alloys elasticity hardness...
Abstract
View article
PDF
ASTM B 752 GRADE 702C is a zirconium casting alloy. Zirconium alloys are extremely corrosion resistant. They are expensive, but in some cases are superior in corrosion performance to stainless steels, nickel alloys, and titanium. The largest application for zirconium castings is handling hydrochloric acid. Grade 702C is one of the common casting grades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: ZR-11. Producer or source: ATI Wah Chang, Allegheny Technologies.
Journal Articles
Alloy Digest (2003) 52 (11): Zr-12.
Published: 01 November 2003
... treating, machining, and joining. Filing Code: ZR-12. Producer or source: ATI Wah Chang, Allegheny Technologies. Producer or Source: ATI Wah Chang, Allegheny Technologies Copyright © ASM International® 2003 2003 ASM International ASTM B 752 Grade 705C Cast zirconium alloys chemical...
Abstract
View article
PDF
ASTM B 752 Grade 705C zirconium casting alloy is basically identical in composition and similar in properties to its wrought equivalent, UNS R60705, which is grade 705. Zirconium alloys are expensive, but are more corrosion resistant than stainless steels, nickel alloys, and titanium. The largest application for zirconium alloys is in the handling of hydrochloric acid. Grade 705C is one of the common casting grades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: ZR-12. Producer or source: ATI Wah Chang, Allegheny Technologies.
Journal Articles
Alloy Digest (2003) 52 (2): SS-876.
Published: 01 February 2003
... to general corrosion and stress-corrosion cracking. Allvac and Super Tough are trademarks of ATI Properties, Inc. DOI: 10.31399/asm.ad.ss0876 Specification Equivalents: UNS S13800 AMS 5629, bars, forgings, rings, and extrusions AMS 5864, plate General Characteristics: Allvac 13-8 SuperTough alloy...
Abstract
View article
PDF
Allvac 13-8 Super Tough alloy is a modification of the standard Allvac 13-8 alloy. (See Alloy Digest SS-866, November 2002.) It has good fabricability and can be age hardened by a single treatment in the range 510 to 621 deg C (950 to 1150 deg F). Cold working prior to aging enhances the aging. These properties supplement the superior fracture toughness and Charpy impact energies. This martensitic precipitation-hardening stainless steel has very good resistance to general corrosion and stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-876. Producer or source: Allvac.
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-139. Producer or source: ATI Allvac. Producer or Source: ATI Allvac Copyright © ASM International® 2006 2006 ASM International ALLVAC Titanium-6Aluminum...
Abstract
View article
PDF
Allvac Titanium Alloy 6Al-7Nb uses niobium to stabilize the beta phase. It is very similar to Ti-6Al-4V and is widely used in medical and surgical device applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-139. Producer or source: ATI Allvac.
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... strength and ductility, good weldability, good hot and cold workability, and good machinability. Allcorr and Allvac are registered trademarks of ATI Properties, Inc. Fig. 1 Effect of cold work on mechanical properties Fig. 2 Effect of elevated temperature on mechanical properties DOI: 10.31399...
Abstract
View article
PDF
Allcorr (UNS N06110) is a single-phase, non-age-hardenable, nickel-base alloy for service in highly corrosive environments. It is characterized by outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress-corrosion cracking. The alloy has high strength and ductility, good weldability, good hot and cold workability, and good machinability. This datasheet provides information on composition, physical properties, microstructure, tensile properties. It also includes information on high temperature performance and corrosion resistance as well as joining. Filing Code: Ni-600. Producer or source: Allvac Metals Company.
Journal Articles
Alloy Digest (2003) 52 (3): Ni-605.
Published: 01 March 2003
... is a niobium-containing ' precipitate. Allvac and 718-OP are registered trademarks of ATI Properties, Inc. Fig. 1 Thermal conductivity Fig. 2 Linear coefficient of thermal expansion DOI: 10.31399/asm.ad.ni0605 Weldability: Satisfactory welds can be produced in both the solution-treated and fully- aged...
Abstract
View article
PDF
Allvac 718-OP is a versatile alloy that is vacuum induction melted followed by a consumable melting process. The alloy is a special chemistry vacuum melted version of standard Allvac 718. It is a precipitation-hardenable, nickel-base alloy that can be used from -253 deg C (-423 deg F) to 704 deg C (1300 deg F). The main hardening constituent is a niobium-containing gamma prime precipitate. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-605. Producer or source: Allvac Metals Company.
Journal Articles
Alloy Digest (2007) 56 (3): Ni-647.
Published: 01 March 2007
.... The triple melting produces a stronger alloy with consistent properties in strength, stability, and forgeability. Allvac is a registered trademark and Allvac Plus is a trademark of ATI Properties, Inc. Fig. 2 Linear coefficient of thermal expansionFig. 1 Thermal conductivity Mechanical Properties: See Fig. 3...
Abstract
View article
PDF
Allvac 718Plus alloy is a variant of alloy 718 (Alloy Digest Ni-90, April 1964) made by adding new elements and adjusting others. The triple melting produces a stronger alloy with consistent properties in strength, stability, and forgeability. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-647. Producer or source: Allvac, an Allegheny Technologies Company.
Journal Articles
Alloy Digest (2005) 54 (7): Ti-136.
Published: 01 July 2005
... remelting (VAR) furnace to minimize segregation. The alloy has a unique combination of properties and is used in the medical, chemical, and aerospace industries. Allvac is a trademark of ATI properties. Table 1 Mechanical Property Data Tensile strength, Yield strength, Thickness, min 0.2% offset, min...
Abstract
View article
PDF
Allvac Ti-15Mo is a metastable beta alloy melted in a vacuum arc remelting (VAR) furnace to minimize segregation. The alloy has a unique combination of properties and is used in the medical, chemical, and aerospace industries. This datasheet provides information on composition. Filing Code: TI-136. Producer or source: Allvac, an Allegheny Technologies Company.