Alloy Digest (2003) 52 (10): Zr-11.
Published: 01 October 2003
... ASTM B 752 GRADE 702C is a zirconium casting alloy. Zirconium alloys are extremely corrosion resistant. They are expensive, but in some cases are superior in corrosion performance to stainless steels, nickel alloys, and titanium. The largest application for zirconium castings is handling...
Journal Articles
Alloy Digest (2003) 52 (11): Zr-12.
Published: 01 November 2003
... ASTM B 752 Grade 705C zirconium casting alloy is basically identical in composition and similar in properties to its wrought equivalent, UNS R60705, which is grade 705. Zirconium alloys are expensive, but are more corrosion resistant than stainless steels, nickel alloys, and titanium. The largest...