Alloy Digest (2003) 52 (11): Ti-132.
Published: 01 November 2003
... ASTM B 367 GRADE Ti-Pd8A is commercially pure titanium casting alloy with a small palladium addition. For the most part, titanium casting alloys are based on traditional wrought product compositions. The small palladium addition to this grade improves corrosion resistance while not changing any...