Alloy Digest (1990) 39 (7): SA-448.
Published: 01 July 1990
... ASTM A572 covers low-alloy, high-strength steels of four different yield strength levels, 42, 50, 60 and 65 ksi. Strengthening is provided by small additions of columbium, vanadium, columbium+vanadium or vanadium+nitrogen. Maximum carbon is at 0.21 to 0.26%, depending on thickness, as shown...
Journal Articles
Alloy Digest (2008) 57 (4): SA-578.
Published: 01 April 2008
... elongation, %, for T-Star plates Specification Equivalents: ASTM A36 ASTM A572, Grades 42, 50 ASTM A709, Grade 50 General Characteristics: T-Star is a high-strength low-alloy (HSLA), multipurpose structural plate grade produced to meet the requirements of ASTM A36 or A572. T-Star, depending on thickness...
Journal Articles
Alloy Digest (1989) 38 (7): SA-438.
Published: 01 July 1989
... be preheated to at least 70°F and held at that temperature during welding Specification Equivalent: ASTM A572 Grade 50. Manufacturer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016. DOI: 10.31399/asm.ad.sa0436 Copyright © ASM International® 1996 Table 3 -- WEIGHT AND SECTION PROPERTIES OF BETHLEHEM...
Journal Articles
Alloy Digest (2016) 65 (1): SA-740.
Published: 01 January 2016
... or better after 40 h in AASS test. The same rating will be achieved in NSS test after about 100 h. Specification Equivalents: EN 20MnV6 DIN 20MnV6 BS 55M AFNOR E420 ASTM A572 General Characteristics: This material is based on a low carbon, microalloyed steel combining high strength with excellent...