Alloy Digest (1990) 39 (3): CS-126.
Published: 01 March 1990
... ASTM A 36 defines the primary or basic structural steel for construction. The specification covers rolled carbon steel for structural purposes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on machining and...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (1987) 36 (8): Fe-79.
Published: 01 August 1987
... NILO alloy 36 is a binary iron-nickel alloy having a very low and essentially constant coefficient of thermal expansion at atmospheric temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... chloride type fluses are used as flux for remelting for casting. DOI: 10.31399/asm.ad.al0066 Copyright © ASM International® 1996 Specification Equivalents: ASTM AUoy SGlOOA-B SAE 309 Aluminum 360 & A360 Fed. QQ-A-591a-1 Camp. 12 MIL-A-15153a Cl. 9 m-A-8294 Comp. 2 General Characteristics: Apex 36 has good...
Journal Articles
Alloy Digest (2012) 61 (4): Fe-159.
Published: 01 April 2012
... Supra 36 is a Fe-Ni alloy with 36% nickel content that exhibits the highest electrical resistivity in the Fe-Ni system. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining...
Journal Articles
Alloy Digest (1989) 38 (11): P-12.
Published: 01 November 1989
... temperatures and oxidation resistance. They cure rapidly to give fast green strength and superior creep resistance. *DERAKANE is a registered trademark of The Dow Chemical Company. Chemical Chaacterization: DEFUKANE 470-36 and 470-45 vinyl ester resins with double bonds confined to the ends of the molecular...
Journal Articles
Alloy Digest (1954) 3 (6): SA-19.
Published: 01 June 1954
... ASTM-WC1 is a molybdenum alloy steel recommended for castings for pressure containing parts suitable for high temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It...
Journal Articles
Alloy Digest (1985) 34 (2): SA-406.
Published: 01 February 1985
... STROLOY 503-A is a hypereutectoid steel of bearing quality. It has through-hardening characteristics similar to those of AISI 52100 steel. Stroloy 503-A is made in accordance with ASTM A 295-84. It is used principally in ball bearing applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1972) 21 (10): SA-281.
Published: 01 October 1972
...: STROLOY 503-A is a through-hardening bearing steel with a nominal carbon analysis of 0.97%. It is made by the electric-furnace process, vacuum carbon deoxidized prior to teeming and conforms to ASTM specification A-295-70 with the exception of Chemical Composition and Analysis (paragraph 3). It has high...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... results in residual stresses, a suitable stress-relieving heat treatment should be applied. Specification Equivalents UNS C51000 EN CW451K ASTM Flat Products B100, B103 DOI: 10.31399/asm.ad.cu0871 Producer Gebr. Kemper GmbH + Co. KG Metallwerke D-57462 Olpe, Germany Tel: +49 (0) 2761 891 0 Fax +49 (0...
Journal Articles
Alloy Digest (1955) 4 (11): Ti-8.
Published: 01 November 1955
... Resistance: Rem-Cru A-1lOAT alloy is una&xd after 1000 hours in the standard ASTM salt spray test Essenridy, corrosion re- sistance characteristics of this grade are similar to those of commercially pure riranium. Cleaning: Descaie in wandand sodium hydride or Hooker bath, followed by water quench and brief...
Journal Articles
Alloy Digest (1979) 28 (6): SS-365.
Published: 01 June 1979
... grain size of 5 or finer. when measured in accordance with ASTM E 112. The alloy shows no banding or duplex grain structure. Machining: The same techniques and equipment are used for machining Techalloy A-286 as for the AISI 300 series stainless steels. Since it is gummy in the soft, solution-treated...
Journal Articles
Alloy Digest (2020) 69 (12): CI-76.
Published: 01 December 2020
... ISO 185/JL/250 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 250–350 MPa (36–51 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Journal Articles
Alloy Digest (1956) 5 (3): Cu-36.
Published: 01 March 1956
... HERCULOY 421, also known as Revere Alloy No. 421, is a low silicon bronze having tensile properties comparable to cartridge brass and corrosion resistance similar to that of copper This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1958) 7 (1): Mg-36.
Published: 01 January 1958
..., fluorides, chromates and di- chromates. Other acids and aqueous salt solutions attack the alloy to a varying degree. Specification Equivalents: ASTM B93-56T AZ91B ASTM B94-52 AZ9lB SAE 501A General Characteristics: Magnesium AZ91B composition shown is the standard composition generally used. This standard...
Journal Articles
Alloy Digest (1964) 13 (1): Co-36.
Published: 01 January 1964
... properties tensile properties Wallex no. 6 WALLEX No. 6 Filing Code: Co-36 Cobalt Alloy JANUARY 1964 -DATA ON WORLD WIDE METALS AND ALLOYS Published by WALLEX No. 6 engineering Alloys Digest. Inc. (Hard Facing Alloy) Upper Montchir. Near Jw Wallex No. 6 is a cobalt-base alloy recommended for hard...
Journal Articles
Alloy Digest (2008) 57 (1): Fe-143.
Published: 01 January 2008
... Invar is an Fe-Ni alloy with 36% Ni content that exhibits the lowest expansion of known metals from very low temperatures up to approximately 230 deg C (445 deg F). Invar M93 is a cryogenic Invar with improved weldability. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2021) 70 (5): CI-81.
Published: 01 May 2021
... Meehanite GD250 is an intermediate-tensile-strength, pearlitic gray cast iron grade that has a minimum tensile strength of 250 MPa (36 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Owing to its good machinability it is suitable for mass...
Journal Articles
Alloy Digest (2013) 62 (6): TS-718.
Published: 01 June 2013
... DIMO 2311 is a modified version of 1.2311 according to Stahl-Eisen Liste and similarly, a modified version of AISI P20 according to ASTM A681. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing...
Journal Articles
Alloy Digest (2013) 62 (7): TS-719.
Published: 01 July 2013
... DIMO 2312 is a modified version of 1.2312 according to Stahl-Eisen Liste and similarly, a modified version of AISI P20 according to ASTM A681. The alloy is sulfurized for machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes...