... STORA ASP 23 high-speed tool steel offers very good abrasion resistance and resistance to softening at elevated temperatures. The excellent size stability and good grindability of this steel make it highly suitable for tools of complicated shape, such as hobs, broaches and threading dies. The high...
Journal Articles
Alloy Digest (1991) 40 (3): TS-503.
Published: 01 March 1991
... ASP 23 is a high-speed tool steel manufactured by the ASP powder metallurgy process in which the steel is atomized, compacted, and hot formed to the desired dimensions. This datasheet provides information on composition, physical properties, hardness, elasticity, and bend strength. It also...
Journal Articles
Alloy Digest (1954) 3 (2): Mg-8.
Published: 01 February 1954
... aioIsaceptrharthetoprakeshouIdbereduc~ito3-8deg. Use cememud-cubidc took wherever possibk aspe&iIy on produaion jobs employing eutmmeIy high cutting spaads. SmaIIer rake angks shodd be used with carbide mols than with high speed seed co prevent chipping and ro provide moresupportforthealaingedge.sincemn,gncsmmaIIoys produce a Iarge...