Skip Nav Destination
Close Modal
Search Results for
ASARCOLO 217-440
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
ASARCOLO 217-440
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (1): Bi-2.
Published: 01 January 1978
... ASARCOLO 158-190 and 217-440 are non-eutectic alloys that can be melted easily. Each range indicates the range through which the alloy melts; thus ASARCOLO 158-190 is a non-eutectic alloy that has a melting range from 158 F to 190 F and ASARCOLO 217-440 is another non-eutectic alloy that melts...
Abstract
View article
PDF
ASARCOLO 158-190 and 217-440 are non-eutectic alloys that can be melted easily. Each range indicates the range through which the alloy melts; thus ASARCOLO 158-190 is a non-eutectic alloy that has a melting range from 158 F to 190 F and ASARCOLO 217-440 is another non-eutectic alloy that melts in the range 217 F to 440 F. These alloys are used widely to aid foundry and machine shop practices, for anchoring components, to spot fixtures for awkward shapes, and for soldering. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Bi-2. Producer or source: Federated Metals Corporation, ASARCO Inc..