Alloy Digest (1971) 20 (2): SA-260.
Published: 01 February 1971
... ARMCO VNT is a high-strength, low-alloy steel normalized for added toughness, ductility and uniformity. It is a silicon-killed, vanadium-nitrogen treated steel, made to fine-grain practive and provides a 60,000 psi minimum yield strength. This datasheet provides information on composition...