Alloy Digest (1989) 38 (10): SS-75.
Published: 01 October 1989
... or Source: Armco Advanced Materials Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International ARMCO PH15-7Mo chemical composition corrosion-resistant alloys creep properties elasticity heat treatability high-temperature alloys joinability physical properties tensile...
Journal Articles
Alloy Digest (1966) 15 (6): SS-183.
Published: 01 June 1966
..., it approximates the austenitic chromium- nickel types of stainless steel. In Condition CH 900, its general corrosion resistance is comparable to that of the austenitic chromium-nickel grades in most media. Irs resistance to stress cracking or stress corrosion is superior to rhac of Armco PH15-7Mo. Stress...