... ARMCO NITRONIC 50 STAINLESS STEEL provides a combination of corrosion resistance and strength not found in any other commercial material available in its price range. It has good mechanical properties at both elevated and sub-zero temperatures. It does not become magnetic when cold worked...
Journal Articles
Alloy Digest (1990) 39 (7): SS-308.
Published: 01 July 1990
... ARMCO NITRONIC 60 Stainless Steel provides outstanding galling and wear resistance. It also has excellent high-temperature oxidation resistance and low-temperature impact resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1990) 39 (8): SS-327.
Published: 01 August 1990
... ARMCO NITRONIC 40 Stainless Steel is one of the most versatile austenitic stainless steels with a room-temperature yield strength about twice that of AISI Types 304, 321 and 347. In addition, NITRONIC 40 has remarkably good elevated temperature properties and oxidation resistance. It retains high...
Journal Articles
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
.... Inc. I201-677.9161 27 CarhId Street. Orange. N.J. 0706Ol USA NITRONIC 30 NITRONK? 30 is a nitrogen-strengthened stainless steel with a good combination of strength, corrosion and wet abrasive wear resistance and economy. Nitron? a registered trademark of Armco, Inc. Composition, Wt. %: Physical...
Journal Articles
Alloy Digest (1976) 25 (1): SS-324.
Published: 01 January 1976
... against a Rockwell C 64 carburized ring in an LFW-1 machine gave the following results: MOY Hardness Wear Index* Type 440C RC59 0.003 Nitronic 33 RB92 0.30 Type 410 Armco 174 PH Type 304 gi 0.30 0.47 1 .oo *Smaller numbers indicate less wear. The galling resistance of Nitronic 33 stainless steel also...
Journal Articles
Alloy Digest (1975) 24 (11): SS-320.
Published: 01 November 1975
... 304 stainless steel and comparable corrosion resistance. It is used in such applications as fasteners, springs, antennae, shafting and pole-line hardware. *NITRONIC is a trademark of Armco Steel Corporation. Composition: Carbon Manganese Silicon Chromium Nickel Nitrogen Iron Typical 0.10 12.00 0.50...
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... that is 3 to 4 times that of type 3 16 stainless steel. ~rmco and Niuonic are registered trademarks of Armco, Inc. The alloy is covered under U.S. Patent 3.912,503. Inconel is a trademark of the Into family of companies. Chemical Composition, wt z szl all-omim Nrkel Molybhum Physical Properties: Density. kg...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
... protection. Nitronic alloys are produced by ElectraBoy under license from Armco Inc. Additional data can be found in Alloy Digesr SS-308. Product Forms Available: EkctraUoy Nitxonic 60 stainless steel is available in bar, master alloy pigs, ingots, and forging quality billets. Applications: Gutstanding...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
... of stainless steel coupons) Weight loss, mg/1000 cycles Alloy 304 at HRB 99 316 at HRB 91 17-4PH at HRC 43 Nitronic 32 at HRB 95 Nitronic 50 at HRB 99 Nitronic 60 at HRB 96 440C at HRC 57 304 12.8 316 10.5 12.5 17-4 24.7 18.5 52.8 Nitronic 32 8.4 9.4 17.2 7.4 Nitronic 50 9.0 9.5 15.7 8.3 10.0 Nitronic 60 6.0...
Journal Articles
Alloy Digest (1998) 47 (11): SS-724.
Published: 01 November 1998
...~aavcrageoffiveSSh~. Specimenslestedar35and80oCwerrintendonallyacrivaredfarherhirdf~~ ~periods.w&rc~activeandpassivtpen~occllrrcdonlyacriverarcs~sbavn Specification Equivalents: ASTM A 35 1 and A 743 (Grade CG6Mh4N) General Characteristics: Nitronic 50 is an austenitic stainless steel that provides a combi- nation...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1025.
Published: 01 December 2008
... CARLSON ALLOY NITRONIC® 50 (High-Manganese Austenitic Stainless Steel) Carlson Alloy Nitronic® 50 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. It possesses good mechanical properties at both elevated and subzero temperatures, and retains low...
Journal Articles
Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
..., and other stainless steels, Nitronic 33 has economic, fabricating, and engineering advantages for cryogenic use. It is easily welded and does not require post or preheat treatments. It is char- acterized by very high strength at subzero temperatures, yet it maintains a high level of ductility and structural...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1228.
Published: 01 October 2015
.... Fabricability: Although this has higher yield strength than Type 304, this alloy may be formed on the same fabricating equipment, CARLSON ALLOY NITRONIC® 40 (High Manganese Austenitic Stainless Steel) Filing Code: SS-1228 Stainless Steel :: October 2015 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax...
Journal Articles
Alloy Digest (1998) 47 (8): SS-727.
Published: 01 August 1998
... toughness and creep. It also includes information on high temperature performance as well as casting and heat treating. Filing Code: SS-727. Producer or source: Various stainless steel casting companies. Producer or Source: Various stainless steel casting companies Copyright © ASM International® 1998...
Journal Articles
Alloy Digest (1996) 45 (12): SS-663.
Published: 01 December 1996
... to Type 409 stainless steels in weld formabiity and toughness. Applications include coal-handling equipment. transportation containers, mixers, liners, exhaust flanges. beat shields, and cyclones. Annco and Nitronic are registered trademarks of Armco Inc. Astralloy V is a registered trademark of Havsco...
Journal Articles
Alloy Digest (1977) 26 (4): SS-338.
Published: 01 April 1977
... AQUAMET 22 is an austenitic stainless steel with an outstanding combination of strength, toughness and corrosion resistance. Its corrosion resistance is equal to or better than any other boat shafting material, even better than most high-nickel alloys. It is the best material available...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... stainless steel having seawater corrosion resistance better than AISI Type 304 and approaching that of AISI Type 316 stainless steel. Its good strength and super toughness make it an ideal material for pleasure and work boats. *AQUAMET is a registered trademark of Armco Steel Corporation. Composition...