Alloy Digest (2000) 49 (5): SS-783.
Published: 01 May 2000
... Armco 440A is a martensitic hardenable, high-carbon, high-chromium stainless steel recommended for cutlery, valve parts, and surgical instruments. It is always used in the hardened condition. This datasheet provides information on composition, physical properties, elasticity, and tensile...