1-15 of 15 Search Results for

ARMCO 17-14

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1958) 7 (1): SS-68.
Published: 01 January 1958
... ARMCO 17-14 Cu-Mo is an austenitic stainless steel which responds favorably to an age-hardening heat treatment. It is recommended for highly stressed stainless steel parts requiring long service at temperatures up to 1500 F. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1989) 38 (11): SS-204.
Published: 01 November 1989
... 114000 H 1150-M 104000 1OOOOO 96000 88000 Elongation,%in4xDor2 H925 16 15 14 15 H 1025 17 15 14 15 H 1100 19 16 14 14 H 1150-M 23 20 19 17 Reduction of area, 8 H 925 59 54 59 60 H 1025 64 58 57 60 H 1100 67 62 57 60 H 1150-M 75 64 70 69 Properties in Tables 1 and 2 are averages of 4 duplicate tests; 2...
Journal Articles
Alloy Digest (1989) 38 (9): SS-7.
Published: 01 September 1989
... ARMCO 17-4 PH, a precipitation hardening stainless steel, is widely accepted in a broad range of industries. High strength, excellent corrosion resistance, ease of heat treatment and good weldability make it an important alloy to designers and engineers. This datasheet provides information...
Journal Articles
Alloy Digest (1989) 38 (5): SS-3.
Published: 01 May 1989
... ARMCO 17-7 PH is a precipitation-hardening stainless steel that provides high strength and hardness, excellent fatigue strength, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition, then hardens to high strength levels by simple heat...
Journal Articles
Alloy Digest (1988) 37 (8): Fe-84.
Published: 01 August 1988
... Rockwell B (equivalent) 76 ASTM ARMCO Table 2 --MAXIMUM CORE LOSS LIMITS* 60 HERTZ 50 HERTZ coreLo9s ORIENTED Thickness 15 k gausses 17 k gausses 15 K gausses 17 k gauss- Type Grade in. (mm) Wnb Wk W/lb w&3 Wnb Wk wnb Wlb 18GO42 M-2 0.007 (0.18) 0.42 0.93 7 7 0.32 0.70 7 7 236046 M-3 0.009 (0.23) 0.46 1.01...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
.... Specification Equivalents: ASTM A 5 14 (Grade D) and A 5 17 (Grade D). ASME SA-5 17 (Grade D). AMS 6386. General Characteristics: The high strength of Armco SSS 1OOA is achieved through a balanced chemical composition and heat treatment. Both chromium and molybdenum promote hardenability, enhance atmospheric...
Journal Articles
Alloy Digest (1968) 17 (12): SA-234.
Published: 01 December 1968
... y; and less 90000 17 50 235-293 7270@ 72500 58800-75600 90000 16 45 235-293 72700 72500 58800-75600 Table 2 - JOMINEY H.\RDENABILITY (Distance from quenched end in 1 16 inch) ,J Distance 1 2 3 4 6 8 10 12 14 16 24 32 Rc max. 46.7 47.0 47.0 46.8 46. 45.5 44.5 43.3 42.2 41.0 Rc min. 41.8 41.0 40.5...
Journal Articles
Alloy Digest (1990) 39 (2): SS-224.
Published: 01 February 1990
...- complished in low-dew point hydrogen, helium or argon atmos- pheres or in vacuum. Machinability: Armco PH 13-8 MO stainless in Condition A provides good tool life and surface finish at machining speeds 20 to 30% lower than Tem~rawrc - F types 410 and 431 but is somewhat inferior to Atmco 17-4 PH stainless...
Journal Articles
Alloy Digest (1963) 12 (7): SS-145.
Published: 01 July 1963
... Armco 410 Cb is a modified Type 410 corrosion resistant steel by the addition of columbium. It is extremely tough and impact resistant. It is a hardenable grade but less sensitive to tempering variables than Type 410. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
...-180000 Yield strength, psi (0.2%) ~gNJ-WO 165000-200000 175ooo 80000-110000 Proportional limit, psi 95ooo-135ooo - Elongation, % in 2 6-15 8-17 14 Reduction of area, % 30-60 30-60 Rockwell hardness c3o-35 c40-45 C:: lrod impact, ft. lbs. c40-45 IO-40 25 10-20 Endurance srrengch, psi 10 million cycles...
Journal Articles
Alloy Digest (1962) 11 (7): SS-134.
Published: 01 July 1962
... ESCO Alloy 36PH is a cast copper containing Fe-Cr-Ni precipitation hardening stainless alloy. It is the cast counterpart of the familiar Armco 17-4PH precipitation hardening alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
...) 21 (3) 262 (38) H 950 (415), 17-4PH 21 (3) 14 (2) 21 (3) 21 (3) 14 (2) 14 (2) 14 (2) 14 (2) 345 (50)(b) 345 (50)(b) Ann (235), Nitronic 32 317 (46) 310 (45) 55 (8) 345 (50)(b) 345 (50)(b) 207 (30) 21 (3) 345 (50)(b) 207 (30) 345 (50)(b) Ann (205), Nitronic 60 345 (50)(b) 345 (50)(b) 248 (36) 345 (50...
Journal Articles
Alloy Digest (1998) 47 (5): SS-716.
Published: 01 May 1998
... 50 T 1613 234 1772 257 I2 52 2330 338 132 50 Ii950 L 16rn 235 1751 254 14 63 24% 362 1.43 49 T 15% 230 1724 x0 I2 53 2448 355 I .42 49 HlOCO L 14% 217 1593 231 I5 65 2427 352 15.? 47 T 1455 21 I 1565 227 15 2406 1.54 47 HIW L 1407 204 1503 218 17 :; 2365 E I .57 46 T 1407 204 1503 218 16 61 2351 341...
Journal Articles
Alloy Digest (1954) 3 (8): SS-17.
Published: 01 August 1954
... as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: SS-17. Producer or source: Donegal Manufacturing Corporation. Producer or Source: Donegal Manufacturing Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International castability chemical...
Journal Articles
Alloy Digest (1965) 14 (5): SS-168.
Published: 01 May 1965
... Condition psi psi (0.2%) % in 2 Hardness A 130000 40000 35 885 TH&I50 200000 145 100000 85 ; C31 43 C H;OO 220000 170000 C43 265000 260000 : c47 A1750 133000 42000 17 B85 R-100 175000 115000 9 RH950 sheer 235000 220000 6 E:t & strip RH750 plare 215000 195000 9 c47 Table 2 - TYPICAL RELAXATION PROPERTIES...