Alloy Digest (1986) 35 (2): SS-424.
Published: 01 February 1986
... ARMCO 12 SR was developed specifically for automotive exhaust applications. It has greater oxidation resistance than AISI Type 409 and it exhibits formability and weldability comparable to more highly alloyed ferritic grades. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1971) 20 (9): SS-259.
Published: 01 September 1971
... 446 also were exposed in the annealed condition at 8850F up to 3000 hours. Both materials exhibited embrittlement at approximately 12 to 24 hours. Armco 18 SR appears to behave in a manner similar to Type 446 with regard to 8850F embrittlement. Armco 18 SR and Type 446 also were exposed...