1-1 of 1 Search Results for

ARMCO 11 Cr-Cb STAINLESS STEEL

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1997) 46 (7): SS-690.
Published: 01 July 1997
... Armco 11 Cr-Cb stainless steel has higher silicon content and is dual stabilized with titanium and columbium (niobium). The alloy is designed for use in automotive exhaust systems and should be considered where the performance of AISI Type 409 stainless steel is marginal. This datasheet provides...