1-5 of 5 Search Results for

APEX TERNALLOY 7

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... APEX TERNALLOY 7 is one of a family of three APEX TERNALLOYS; see also APEX TERNALLOY 5 (Alloy Digest A1-273, revised March 1987) and APEX TERNALLOY 6 (Alloy Digest A1-277, February 1987). It can be hardened by aging at room temperature without a solution treatment and offers high mechanical...
Journal Articles
Alloy Digest (1954) 3 (8): Al-19.
Published: 01 August 1954
... on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-19. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical composition corrosion...
Journal Articles
Alloy Digest (1987) 36 (2): Al-277.
Published: 01 February 1987
... APEX TERNALLOY 6 is one of a family of three APEX aluminum casting alloys (See APEX TERNALLOY 5, A1-273, November 1986.). It can be hardened by aging at room temperature and offers high mechanical properties. It has good castability, excellent machinability and high resistance to corrosion. Its...
Journal Articles
Alloy Digest (1987) 36 (3): Al-273.
Published: 01 March 1987
... properties UNS A07050 I *-mu m--mm m I m a-7 I 5 Filing Code: Al-273 Aluminum Alloy -s--w N Revised MARCH 1987 NOVEMBER 1986 -- - -- I w-w - 1OYS Published hr Alloy Digest. inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 APEX TERNALLOY* 5 (Aluminum Foundry Alloy) APEX TERNALLOY 5 is one...
Journal Articles
Alloy Digest (1952) 1 (1): Al-1.
Published: 01 September 1952
...: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical composition corrosion-resistant alloys hardness heat treatability joinability machinability physical properties sand castings tensile...