Alloy Digest (1987) 36 (3): Al-273.
Published: 01 March 1987
... APEX TERNALLOY 5 is one of three Apex aluminum casting alloys. Its strength, toughness and excellent machining and finishing characteristics give it applicability for both functional and decorative parts. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1987) 36 (2): Al-277.
Published: 01 February 1987
... APEX TERNALLOY 6 is one of a family of three APEX aluminum casting alloys (See APEX TERNALLOY 5, A1-273, November 1986.). It can be hardened by aging at room temperature and offers high mechanical properties. It has good castability, excellent machinability and high resistance to corrosion. Its...
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... APEX TERNALLOY 7 is one of a family of three APEX TERNALLOYS; see also APEX TERNALLOY 5 (Alloy Digest A1-273, revised March 1987) and APEX TERNALLOY 6 (Alloy Digest A1-277, February 1987). It can be hardened by aging at room temperature without a solution treatment and offers high mechanical...
Journal Articles
Alloy Digest (1955) 4 (6): Al-27.
Published: 01 June 1955
... TERNALLOY 5 is a room temperature aging aluminum-magnesium-zinc casting alloy offering high mechanical properties in the cast and aged condition, good castability and high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1954) 3 (8): Al-19.
Published: 01 August 1954
..., gasoIi0eha0diiog equipmenr, pressure V&ICS aansmission hotlsings. washing mat&& agi- cacors, fitrings, eta2 Manufacturer: Apex Smelting Company chicago, uinois; Cleveland, Ohio; and Los Angeles, California 1 Or DIGEST CARPENTER No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS Publisbcd...
Journal Articles
Alloy Digest (1952) 1 (1): Al-1.
Published: 01 September 1952
...& components, housings. geats, machinm parrs, manifoids. gasoline-hzodling cquipm~t, transmission housings, washing machine agitators, kings, etc. Apex Smelting Company Chicago, Iiliaois and Cleveland, Ohio 1 Or DIGEST CARPENTER No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1957) 6 (11): Al-59.
Published: 01 November 1957
... treating, machining, and joining. Filing Code: Al-59. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright Ā© ASM InternationalĀ® 1996 1996 ASM International castability chemical composition corrosion-resistant alloys elasticity hardness heat...