Alloy Digest (1956) 5 (10): Mg-28.
Published: 01 October 1956
... APEX 910 is a magnesium die casting alloy containing about 9% aluminum. It combines good mechanical properties, good casting characteristics, and good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1955) 4 (5): Mg-17.
Published: 01 May 1955
... MIL Aero AN-M-16 MIL-M-4204 Navy 46MM Army 57-74-3 AMS 4490 AZ91 Alcoa 263 Apex 910 Elekuon AZ91 Domar Az91x Canadian CSA HGll General Characteristics: Dowmecal R and RC are general die casting alloys. They possess the desirable combination of good cast- ing characteristics and good mechanical...