1-1 of 1 Search Results for

APEX 417

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1958) 7 (1): Al-61.
Published: 01 January 1958
... APEX 417 is an aluminum-magnesium casting alloy having high strength and ductility, excellent corrosion resistance and good dimensional stability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and...