Alloy Digest (2008) 57 (5): Cu-754.
Published: 01 May 2008
... Ansonia alloys C19140 and C19160 are precipitation-hardening alloys. Properties of these alloys are enhanced by additional cold work. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on forming...