Alloy Digest (2009) 58 (3): Cu-767.
Published: 01 March 2009
... Ansonia alloy C65500 and C66100 are high silicon bronze and leaded high silicon bronze alloys that are high strength; the latter are the machinable equivalent. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...