Alloy Digest (2009) 58 (8): Cu-773.
Published: 01 August 2009
... Ansonia alloy C23000 is a 15% Zn alloy with the previous trade name of Red Brass. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...