Skip Nav Destination
Close Modal
Search Results for
ANSONIA ALLOY C15000
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for ANSONIA ALLOY C15000
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2011) 60 (5): Cu-798.
Published: 01 May 2011
... Ansonia alloy C15000 is a 0.15% Zr alloy and is often called zirconium copper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-798. Producer...
Abstract
View articletitled, <span class="search-highlight">ANSONIA</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">C15000</span>: Resistance Electrode <span class="search-highlight">Alloy</span>
View
PDF
for article titled, <span class="search-highlight">ANSONIA</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">C15000</span>: Resistance Electrode <span class="search-highlight">Alloy</span>
Ansonia alloy C15000 is a 0.15% Zr alloy and is often called zirconium copper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-798. Producer or source: Ansonia Copper & Brass Inc..