Alloy Digest (1980) 29 (11): Cu-406.
Published: 01 November 1980
... ANACONDA Alloy 210 has a composition that imparts to it a slightly greater strength than copper, corrosion resistance about the same as copper, and an excellent resistance to stress-corrosion cracking. It has good hot-working properties and excellent cold-working characteristics. Among its many...
Journal Articles
Alloy Digest (1967) 16 (5): Cu-176.
Published: 01 May 1967
... stems, petroleum refinery heat exchangers,propellers, bushings, molds, pickling equipment. Modocturer: Ampco Metals Co., Milwaukee, Wisconsin Anaconda American Brass Co., Waterbury, Connecticut Mueller Brass Co., Port Huron, Michigan and other copper alloy mills. ...