Alloy Digest (1979) 28 (12): Cu-385.
Published: 01 December 1979
... ANACONDA Alloy (E) 505 is a low-tin phosphor bronze with excellent resistance to corrosion, excellent ductility and good resistance to fatigue. It has good thermal and electrical conductivity. Its uses include flexible metal hose, electrical contacts, fuse clips and fasteners. This datasheet...