1-15 of 15 Search Results for

AMPCOLOY C-3

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (6): Cu-334.
Published: 01 June 1977
... AMPCOLOY C-3 is a copper-aluminum-iron alloy with high strength and hardness, good toughness, good resistance to fatigue and wear, and good corrosion resistance. It is used for heavy loads in such applications as bearings, gears and hydraulic valve parts. It is suited for service up to 750 F...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... (% IACS) 30 (52) Thermal conductivity, W/m·K (Btu/h·ft·ºF) 20 °C (68 °F) 230 (133) 100 °C (212 °F) 250 (144) 200 °C (392 °F) 270 (156) Specific heat Cp, J/kg·K (cal/g·ºC) 420 (0.10) Magnetic permeability, µ <1.05 Mechanical Properties: Modulus of elasticity, GPa (106 psi) 130 (18.85) Hardness, HB, 3000 kg...
Journal Articles
Alloy Digest (1976) 25 (3): Cu-310.
Published: 01 March 1976
... 160000 H + age hardened up to 3/8. incl 200000 182000 H + age hardened Over 3/8-l, incl 195000 178000 H + age hardened Over 1 190000 175000 Tensile Strength psi Yield Strength (0.2% Offset) psi Elongation (2 in.) Rockwell Hardness _ % B C -- 48 15 15 95 - 15 95 6 -38 3 -41 5 -41 3 -41 Copyright © ASM...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-383.
Published: 01 November 1979
.... Military: M&C-15345, Alloy 6. SAE: J462b, Alloy C 86300. Ingot No. 424. General Characteristics: Ampcoloy 66 is a copper-base casting alloy classed as High-Strength Yellow Brass. It is usually called High-Strength Manganese Bronze because it is in the high-strength region of the manganese bronzes...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-380.
Published: 01 September 1979
... C96200. ASTM B 369. Military: MIL-B-20159 and MIL-C-15345, Alloy 25. General Characteristics: Ampcoloy 525 is a cast alloy of the 90 copper-IO nickel type. Its nominal composition is actually 87% copper, 10% nickel, 1.5% iron and 1 .O% manganese. The iron is added to increase its resistance to general...
Journal Articles
Alloy Digest (1980) 29 (9): Cu-403.
Published: 01 September 1980
...: Copper Alloy No. C90700. ASTM B 427 (C 907). A!XM B 505 (C907). SAE J462b (C-90700). General Characteristics: Ampcoloy 7 11 is nominally an 89% copper, 11% tin casting alloy that has been deoxidized with phosphorus. It is used in the as-cast condition and cannot be strength- ened by any thermal treatment...
Journal Articles
Alloy Digest (1979) 28 (3): Cu-369.
Published: 01 March 1979
... resistance to most acids and strong alkalies and to cyanides and ammonium compounds. Specification Equivalents: UNS No. C86500. ASTM: B 271 (865) and B 584 (865) - formerly B 147 (865). Federal: QQ-C-390 (C865). Military: MIL-C-15345G, Alloy 4. SAE: J462b (C86500). AMS 46 19 and AMS 4860. General...
Journal Articles
Alloy Digest (1981) 30 (12): Cu-428.
Published: 01 December 1981
... in the presence of moisture. Specification Equivalents: Copper Alloy No. C9 1600. ASTM: B 30 and B 427. Federal: QQ-C-390. Military: M&C-15345 (Alloy 23). UNS No. C91600. Ingot No. 205. General Characteristics: Ampcoloy 54 is nominally an 88.0% copper, 10.3% tin, 1.5% nickel casting alloy that has been deoxidized...
Journal Articles
Alloy Digest (1980) 29 (6): Cu-396.
Published: 01 June 1980
... to most acids and strong alkalies and to cyan- ides and ammonium compounds. Specification Equivalents: ASTM: B 505 and B 584 (formerly B 147), C86200. Federal: QQC-390, C862. CDA Copper Alloy No. C86200. UNS No. C86200. SAE J462b, C-86200. General Characteristics: Ampcoloy 64 is a copper-zinc-aluminum...
Journal Articles
Alloy Digest (1967) 16 (12): Ni-130.
Published: 01 December 1967
... rake angle, deg. S-10 side rake angle, deg. 6-8 side relief angle, deg. 6.8 front relief angle, deg. 5-6 side cutring-edge angle, deg. 10-15 end cutting-edge angle, deg. 10-15 nn~c= rnrli inch 1jR Finishing S-10 6.8 5-6 12-15 lo-15 10-15 Ii16 ...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-408.
Published: 01 December 1980
..., the parts must be rinsed in hot water, dipped into a neutralizing solution, rinsed, and dried in hot air. Specification Equivalents: ASTM B 369 (C96400). ASTM B 505 (C96400). Federal: QQC-390. Military: MIL-C-20159 and MILC-15345G (Alloy 24). CDA Copper Alloy No. C96400. UNS No. C96400. General...
Journal Articles
Alloy Digest (1974) 23 (10): Cu-286.
Published: 01 October 1974
... solution acidified with H2SO4, rinse in hot water and dry- Specification Equivalents: RWMA Group A, Class 3. MlL-C46087(M R) and MIL-C-8 102 1. General Characteristics: Ah4PCOLOY 91 Alloy is an age-hardening copperco- balt-beryllium alloy suitable for many cast and wrought products. It has an excellent...
Journal Articles
Alloy Digest (1963) 12 (5): Cu-128.
Published: 01 May 1963
... although high speed steel tools can be used at lower speeds if necessary. Best results are obcain- ed with Y alenite rypes VC-125 and l C-11, or equivalents. Possesses excellent resistance to corrosion not only in alkaline but also in non-oxidizing acid media. It has excellent corrosion-resistance...
Journal Articles
Alloy Digest (1966) 15 (11): Cu-171.
Published: 01 November 1966
... 327 to420°C Thermal conductivity, cal/cm2/cm/sec/oC at 20°C at 15OoC Electrical resistivity, microhm/cm3 Electrical conductivity, % IACS Modulus of elasticity, psi x 106 Modulus of rigidity, psi x 106 Poisson s ratio PROPERTIES Table 1 - TYPICAL CAST PROPERTIES Sand Cast Centrifugally Cast Tensile...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... (precipi- tation hardened) to med the hardness, strength and &c&al wn- ductivity requirements of the RWMA Class 3 specification. Table 1 gives its mechanical propenies. The heat-treating details are pro prieuuy but will be given to customers who wish to purchase and use the alloy. Machinability: Tile...