1-3 of 3 Search Results for

AMPCOLOY 99

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1976) 25 (7): Cu-315.
Published: 01 July 1976
.... Copyright ┬ę ASM International┬« 1996 1996 ASM International AMPCOLOY 99 chemical composition corrosion-resistant alloys current-carrying rings elasticity electrical conductivity fatigue properties hardness heat treatability joinability machinability physical properties resistance welding...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... Ampcoloy 88 was developed for plastic tooling and has a hardness greater than 260 HB, a high thermal conductivity, with good machinability and polishability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1974) 23 (10): Cu-286.
Published: 01 October 1974
... AMPCOLOY 91 Alloy is a cobalt-bearing copper alloy with a small addition of beryllium to make it age hardenable. It has an excellent combination of strength, toughness and electrical conductivity. It is recommended for resistance welding tips and wheels; flash, butt and projection welding dies...