Alloy Digest (1974) 23 (10): Cu-286.
Published: 01 October 1974
... AMPCOLOY 91 Alloy is a cobalt-bearing copper alloy with a small addition of beryllium to make it age hardenable. It has an excellent combination of strength, toughness and electrical conductivity. It is recommended for resistance welding tips and wheels; flash, butt and projection welding dies...