Alloy Digest (1980) 29 (9): Cu-403.
Published: 01 September 1980
... AMPCOLOY 711 is a medium-strength casting alloy; its typical tensile strength is 55,000 psi in the as-cast condition. It has a good combination of strength, ductility and resistance to corrosion. Among its many uses are bushings, gears, pumps, propellers, valves and marine hardware. This datasheet...