Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... requirements-95,000 psi tensile strength, 90 Rockwell B hardness and 45% IACS electrical conductivity. Potential applications include resistance welding tips, wheels and fixtures. A major use is in plastic injection molding. AMPCO-TRODE 940 is used for repair welding and overlays. This datasheet provides...