Alloy Digest (1993) 42 (11): Cu-591.
Published: 01 November 1993
... AMPCO-TRODE 250 is used in extreme bearing applications and to weld AMPCO 21 castings (See Alloy Digest Cu-93, October 1960). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-591. Producer...
Journal Articles
Alloy Digest (1994) 43 (1): Cu-595.
Published: 01 January 1994
... AMPCO-TRODE 46 is recommended for cast and wrought nickel-aluminum bronze. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-595. Producer or source: Ampco Metal Inc. Producer or Source...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... AMPCO-TRODE 182 is a chromium-copper alloy filler metal that has high conductivity with good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-589. Producer...
Journal Articles
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
... Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 300 chemical composition hardness joinability machinability tensile properties AMpCOJRODE@ 300 k%iy U-596 FEBRUARY 1994 - DIGEST- DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1993) 42 (12): Cu-593.
Published: 01 December 1993
... AMPCO-TRODE 40 is a manganese-nickel-aluminum bronze for welding ship propellers and some dissimilar combinations. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-593. Producer or source...
Journal Articles
Alloy Digest (1993) 42 (8): Cu-586.
Published: 01 August 1993
... AMPCO-TRODE 200 is both filler metal and electrodes for extreme wear and high pressures in bearing overlays. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-586. Producer or source: Ampco...
Journal Articles
Alloy Digest (1993) 42 (7): Cu-585.
Published: 01 July 1993
... AMPCO-TRODE 150 is recommended for overlay application and welding AMPCO 18 alloy (Alloy Digest Cu-51, June 1957). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-585. Producer or source...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... requirements-95,000 psi tensile strength, 90 Rockwell B hardness and 45% IACS electrical conductivity. Potential applications include resistance welding tips, wheels and fixtures. A major use is in plastic injection molding. AMPCO-TRODE 940 is used for repair welding and overlays. This datasheet provides...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
...: Ampco Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition COPPER-TRODE electrical conductivity hardness joinability machinability physical properties tensile properties COPPER-TRODE@ Filing Code: Copper...
Journal Articles
Alloy Digest (1955) 4 (11): Cu-33.
Published: 01 November 1955
... of their greater cooling properties, are recommended as a coolam. Weldabllityz This material is welded quite readily either to like of dissimi!ar merals by ail of the electric-arc methods. From the cost-quality standpoint inert-gas consumable elec- trode process is favored for place. Ampco-Trode 10 fil- ler...
Journal Articles
Alloy Digest (1957) 6 (2): Cu-47.
Published: 01 February 1957
...-arc methods. From the cost-quality standpoint inert-gas consum- able electrode process is favored for plate. Ampco- Trode 10 6ller metal with helium, argon or a mixture is used. The carbon-arc process is also recommended and produces first quality welds with Ampco-Trode 160 coated filler rod...
Journal Articles
Alloy Digest (1957) 6 (6): Cu-51.
Published: 01 June 1957
... readily either m like or dis- similar metals bv all of the electric-arc methods. From the costqualiy s&dpoint inert-gas wnsumable electrode pro- cess is favored for plate. Ampco-Trode 10 6ller metal with helium, argon or a mixture is used. The carbon-arc txoas.5 is also &&unended and produces iirsr...
Journal Articles
Alloy Digest (1976) 25 (7): Cu-315.
Published: 01 July 1976
... properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-315. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc...