1-14 of 14 Search Results for

AMPCO-TRODE 10

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1993) 42 (2): Cu-582.
Published: 01 February 1993
... AMPCO-TRODE 10 is the most versatile aluminum bronze welding electrode in its family and is used for both similar and dissimilar welding. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining. Filing...
Journal Articles
Alloy Digest (1955) 4 (11): Cu-33.
Published: 01 November 1955
... of their greater cooling properties, are recommended as a coolam. Weldabllityz This material is welded quite readily either to like of dissimi!ar merals by ail of the electric-arc methods. From the cost-quality standpoint inert-gas consumable elec- trode process is favored for place. Ampco-Trode 10 fil- ler...
Journal Articles
Alloy Digest (1960) 9 (10): Cu-93.
Published: 01 October 1960
... is favored for plate. Ampco-Trode 10 filler metal with helium, argon or a mixture is used. The carboo-arc process is also recommended and produces first quality welds with Ampco-Trode I60 coated filler rod. Castability: Controlled foundry technique is necessary to accommodate the high shrinkage, short...
Journal Articles
Alloy Digest (1961) 10 (9): Cu-107.
Published: 01 September 1961
... by all of the electric- arc methods. From the cost-quality stand- point inert-gas consumable electrode process is favored for plate. Ampco-Trode 10 filler metal with helium, argon or a mixture is used. The carbon-arc process is also recommended and produces first quality welds with Ampco- Trode 160...
Journal Articles
Alloy Digest (1957) 6 (2): Cu-47.
Published: 01 February 1957
...-arc methods. From the cost-quality standpoint inert-gas consum- able electrode process is favored for plate. Ampco- Trode 10 6ller metal with helium, argon or a mixture is used. The carbon-arc process is also recommended and produces first quality welds with Ampco-Trode 160 coated filler rod...
Journal Articles
Alloy Digest (1957) 6 (6): Cu-51.
Published: 01 June 1957
... readily either m like or dis- similar metals bv all of the electric-arc methods. From the costqualiy s&dpoint inert-gas wnsumable electrode pro- cess is favored for plate. Ampco-Trode 10 6ller metal with helium, argon or a mixture is used. The carbon-arc txoas.5 is also &&unended and produces iirsr...
Journal Articles
Alloy Digest (1965) 14 (10): Cu-156.
Published: 01 October 1965
... Weldability: This material is welded quite readily either to like or dissimilar metals by all of the electric-arc methods, although preheating to approximately 9OOoF is required. From the cost-quality stand- point inert-gas consumable electrode process is favored for plate. Ampco-Trode 10 filler metal...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... AMPCO-TRODE 182 is a chromium-copper alloy filler metal that has high conductivity with good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-589. Producer...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-580.
Published: 01 January 1993
... AMPCO-TRODE 7 is an iron-free aluminum bronze alloy available for overlay welding, particularly surfaces requiring a 125 BHN for wear while being able to resist corrosion from salts and sea water. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1993) 42 (11): Cu-591.
Published: 01 November 1993
... AMPCO-TRODE 250 is used in extreme bearing applications and to weld AMPCO 21 castings (See Alloy Digest Cu-93, October 1960). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-591. Producer...
Journal Articles
Alloy Digest (1993) 42 (6): Cu-584.
Published: 01 June 1993
... is recommended for joining aluminum bronzes (AMFCO 18). ferrous and dissimilar metals requiring higher strength than produced by AMF CO-TRODE 10 FILLER METAL. AMPCO-TRODE 160 aluminum bronze coated elec- trodes produce a deposit of high strength and good ductility with a nominal hardness of 160 Brine11...
Journal Articles
Alloy Digest (1993) 42 (12): Cu-593.
Published: 01 December 1993
... AMPCO-TRODE 40 is a manganese-nickel-aluminum bronze for welding ship propellers and some dissimilar combinations. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-593. Producer or source...
Journal Articles
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
... Metal Inc. Producer or Source: Ampco Metal Inc. Copyright ┬ę ASM International┬« 1996 1996 ASM International AMPCO-TRODE 300 chemical composition hardness joinability machinability tensile properties AMpCOJRODE@ 300 k%iy U-596 FEBRUARY 1994 - DIGEST- DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1976) 25 (7): Cu-315.
Published: 01 July 1976
... properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-315. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc...