Alloy Digest (1957) 6 (2): Cu-47.
Published: 01 February 1957
... AMPCO METAL 20 is an aluminum bronze having high hardness coupled with sufficient ductility suitable for bushings and bearings subjected to heavy presssures and excessive wear. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1979) 28 (6): Cu-374.
Published: 01 June 1979
... or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International acid resisting pumps AMPCO A-1 cast bronze castability chemical composition compressive strength corrosion-resistant alloys elasticity fatigue resistance gears...
Journal Articles
Alloy Digest (1955) 4 (11): Cu-33.
Published: 01 November 1955
... AMPCO METAL-16 is an aluminum bronze combining strength with good elongation, along with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1993) 42 (8): Cu-586.
Published: 01 August 1993
... Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 200 bearing overlays chemical composition hardness joinability machinability tensile properties welding electrodes AMpC@TR()DE@20() i:ed; cu-586 - DIGEST- AUGUST...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-352.
Published: 01 April 1978
... or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO 483 castability chemical composition corrosion-resistant alloys elasticity fatigue resistance hardness heat treatability joinability machinability marine...
Journal Articles
Alloy Digest (2010) 59 (12): Cu-793.
Published: 01 December 2010
... www.ampcometal.com Ampcoloy is a registered trademark of Ampco Metal SA. Table 1 Mechanical properties Property Nominal values Ultimate tensile strength, MPa (ksi) 758 (110) Yield strength, RP 0.5, MPa (ksi) 386 (56) Elongation 2 in., % 16 Brinell hardness, HB 30 207 Rockwell hardness, HRB 95 Reduction of area, % 16...
Journal Articles
Alloy Digest (1983) 32 (12): Cu-469.
Published: 01 December 1983
...-469. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International aerospace components AMPCO M-4 castability chemical composition corrosion-resistant alloys elasticity fatigue resistance hardness heat...
Journal Articles
Alloy Digest (2011) 60 (1): Cu-795.
Published: 01 January 2011
... AMPCO 18.22 and 18.136 are variations of AMPCO 18 to produce a higher ultimate strength and to improve the impact resistance, respectively. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... AMPCO-TRODE 182 is a chromium-copper alloy filler metal that has high conductivity with good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-589. Producer...
Journal Articles
Alloy Digest (1994) 43 (1): Cu-595.
Published: 01 January 1994
... AMPCO-TRODE 46 is recommended for cast and wrought nickel-aluminum bronze. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-595. Producer or source: Ampco Metal Inc. Producer or Source...
Journal Articles
Alloy Digest (1993) 42 (7): Cu-585.
Published: 01 July 1993
...: Ampco Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 150 chemical composition hardness joinability machinability tensile properties AMpC()JR()DEG9150 I cu-585 - DIGEST- JULY 1993 DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
... Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 300 chemical composition hardness joinability machinability tensile properties AMpCOJRODE@ 300 k%iy U-596 FEBRUARY 1994 - DIGEST- DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1993) 42 (11): Cu-591.
Published: 01 November 1993
... or source: Ampco Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 250 chemical composition hardness joinability machinability tensile properties AMpCOJRODE@250 e u-59 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (1955) 4 (2): Cu-23.
Published: 01 February 1955
... AMPCO METAL-8 is a wrought alpha phase aluminum bronze possessing high tensile, impact and faigue characteristics. It is non-magnetic and resistant to sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1958) 7 (6): Cu-64.
Published: 01 June 1958
... and fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-64. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO 15 bearing strength bend...
Journal Articles
Alloy Digest (1993) 42 (12): Cu-593.
Published: 01 December 1993
...: Ampco Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCO-TRODE 40 chemical composition hardness joinability machinability ship propellers tensile properties AM PCO-TRODE@ 40 Filing Code: Copi=r Aiioy cu-593 DECEMBER 1993...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... of Ampco and Ampcoloy materials are based on extensive tests made at the Ampco Metal factories, which also match the values of a great number of customers. Ampcoloy materials are basically easy to machine. Since the cutting speeds depend on the type of cutting tools used, on the stiffness and stability...
Journal Articles
Alloy Digest (1976) 25 (10): Cu-321.
Published: 01 October 1976
..., hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as machining and joining. Filing Code: Cu-321. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: CU-434. Producer or source: Ampco Metal Inc. Originally...
Journal Articles
Alloy Digest (1980) 29 (1): Cu-388.
Published: 01 January 1980
.... This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-388. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco...