Alloy Digest (1983) 32 (12): Cu-469.
Published: 01 December 1983
... AMPCO M-4 is a copper-aluminum-nickel-iron-manganese alloy that possesses high hardness, high strength, good resistance to fatigue and wear, and excellent resistance to corrosion. It is used in both cast and wrought forms. Typical applications include marine hardware, aerospace components, wear...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-580.
Published: 01 January 1993
... machinability physical properties tensile properties thermal properties AMPCO=TRODE@7 Filing Code: Copper Alloy cu-590 JANUARY 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS fiTiZ2E m=-SbkSP- Pdshedby: Aby Digfat. Inc /201%77%161 -(YP-. 27-Sasel.Orange.NJ.070501USA AMPCO-Trade@ 7 (Iron-Free Aluminum...
Journal Articles
Alloy Digest (2010) 59 (12): Cu-793.
Published: 01 December 2010
... ºC (68 ºF), · m ( circular-mil/ft) 1.33x10 4 (0.08) Electrical conductivity, 106S/m (%IACS) 7.5 (13.0) Specific heat capacity, J/kg · K (Btu/lb · ºF) 418.7 (0.1) Mechanical Properties: See Table 1. General Characteristics: This heat-treated alloy is the ultimate in high-strength bronzes requiring...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... of the machine-tools used, and on the type of cooling and lubricating liquids used, the recommended machining speeds for Ampco and Ampcoloy alloys are indicated as relative value compared to the machining speeds used for tools steel 1.7225 (DIN 42 Cr Mo 4). Ampcoloy 88 with a hardness of 260-280 HB 30/10...
Journal Articles
Alloy Digest (2011) 60 (1): Cu-795.
Published: 01 January 2011
... (0.269) Coefficient of thermal expansion, 10 6 /K (10 6/ºF) 16.2 (9.0) Thermal conductivity, 20 ºC (68 ºF), W/m·K (Btu/h·ft·ºF) 59 (34.1) Electrical resistivity, 20 ºC (68 ºF), m ( circular-mil/ft) 1.33 × 10 4 (0.08) Electrical conductivity, 106S/m (%IACS) 7.5 (13.0) Specific heat capacity, J/kg·K (Btu...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... (6.4 mm) deposit 32 (221 Mpa) 14 (97 MPa) 30 60 Applications: Electrical connectors, heater elements, electrode holders, bus bars, crucibles, high-conductivity parts, welding AMPCO 97. Producer: AMPCO Metal, Inc. Milwaukee, WI 53201 4 14-645-3750 DOI: 10.31399/asm.ad.cu0589 Copyright © ASM...
Journal Articles
Alloy Digest (1993) 42 (7): Cu-585.
Published: 01 July 1993
.../4 (6.4 mm) deposit 90 (621 MPa) 40 (276 MPa) 20 22 166 PROPERTIES General Characteristics: AMPCO-TRODE 150 aluminum bronze spooled wire and bare filler rod produce a deposit of high strength and good ductility with a nominal hardness of 166 Brine11 as applied with the inert-gas processes...
Journal Articles
Alloy Digest (1993) 42 (8): Cu-586.
Published: 01 August 1993
... AMPCO-TRODE 200 is both filler metal and electrodes for extreme wear and high pressures in bearing overlays. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-586. Producer or source: Ampco...
Journal Articles
Alloy Digest (1993) 42 (11): Cu-591.
Published: 01 November 1993
..., wear shoes, sheaves, culvert valves, clutch fingers, cable drums, dipper idlers, screw conveyors, cam, mill camps. Producer: AMPCO Metal, Inc. Milwaukee, WI 53201 4 14-645-3750 DOI: 10.31399/asm.ad.cu0591 Copyright © ASM International® 1996 TABLE 2 - MACHINING AMKIO-TRODE 250 TOOL DATA - SPEEDS...
Journal Articles
Alloy Digest (1993) 42 (2): Cu-582.
Published: 01 February 1993
... A5.7 Class ER CuAL42 DOI: 10.31399/asm.ad.cu0582 Copyright © ASM International® 1996 Table 4 -MACHINING AMPCO-TRODE 10 TOOL DATA -SPEEDS AND FEEDS (Conventional Equipment with standard motors) CARBIDE INSERT CEMENTED CARBIDE SLIGHTLY POSTNE HONED EOOE GRIN-D 1 SIDE OF WEB l/32- ALL DRILLS MUST HAVE...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... 209 197 187 150 1% Beryllium-Copper 223 222 211 200 187 134 Nickel-Aluminum Bronxe 178 175 171 162 140 - (Wrought alloy Table 4 - EFFECT OF TEMPERATURE ON ELECTRICAL CONDUCIMTY AND RESISTIVlTY Electrical Conductivity as % lACS and Electrical Resistivity (microhm-cm) at Temperatures of Alloy Ampco 940...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-352.
Published: 01 April 1978
... AMPCO 483 is a copper-base alloy that can be used in the cast or wrought form. It provides high strength, high hardness, excellent resistance to corrosion and good resistance to fatigue and wear. It is well suited for service at temperatures up to 750 F and for applications such as pickling...
Journal Articles
Alloy Digest (1957) 6 (6): Cu-51.
Published: 01 June 1957
... readily either m like or dis- similar metals bv all of the electric-arc methods. From the costqualiy s&dpoint inert-gas wnsumable electrode pro- cess is favored for plate. Ampco-Trode 10 6ller metal with helium, argon or a mixture is used. The carbon-arc txoas.5 is also &&unended and produces iirsr...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
.... Filing Code: CU-789. Producer or source: AMPCO Engineered Alloys. Producer or Source: AMPCO Engineered Alloys Copyright © ASM International® 2010 2010 ASM International Ampcoloy 95 chemical composition hardness machinability physical properties tensile properties welding electrodes...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-383.
Published: 01 November 1979
.... This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-383. Producer or source: Ampco Metal Inc.. Producer or Source...
Journal Articles
Alloy Digest (1980) 29 (9): Cu-403.
Published: 01 September 1980
... provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-403. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
...: Ampco Metal Inc. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition COPPER-TRODE electrical conductivity hardness joinability machinability physical properties tensile properties COPPER-TRODE@ Filing Code: Copper...
Journal Articles
Alloy Digest (1981) 30 (12): Cu-428.
Published: 01 December 1981
... or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCOLOY 54 bearings bushings cast bronze castability chemical composition corrosion-resistant alloys ductility elasticity fittings gears hardness heat...
Journal Articles
Alloy Digest (1966) 15 (11): Cu-171.
Published: 01 November 1966
... or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International Ampcoloy 495 castability chemical composition compressive strength corrosion-resistant alloys creep properties elasticity fatigue properties fracture toughness...
Journal Articles
Alloy Digest (1967) 16 (5): Cu-176.
Published: 01 May 1967
... properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-176. Producer or source: Ampco Metal Inc...