Alloy Digest (1979) 28 (6): Cu-374.
Published: 01 June 1979
... AMPCO A-1 is a cast copper-base alloy well suited for use up to 750 F. It is characterized by fairly high hardness and strength, good resistance to fatigue and wear, and excellent corrosion resistance. Among its many applications are acid-resisting pumps, pickling equipment, gears, marine hardware...
Journal Articles
Alloy Digest (1993) 42 (3): Cu-434.
Published: 01 March 1993
... AMPCO 940 is a precipitation-hardening copper-nickel-silicon-chromium alloy developed for resistance welding and other applications now using the 1% beryllium-copper alloys. The heat-treated alloy is capable of meeting the RWMA (Resistance Welder Manufacturers Association) Class 3 minimum...
Journal Articles
Alloy Digest (2011) 60 (1): Cu-795.
Published: 01 January 2011
.../lb·ºF) 419 (0.1) Mechanical Properties: See Table 1. General Characteristics: By varying the heat treatment and by close control of all operations, the characteristic duplex structure of AMPCO 18 is refined to produce a material AMPCO 18.22 having substantially higher ultimate strength, yield strength...
Journal Articles
Alloy Digest (2010) 59 (12): Cu-793.
Published: 01 December 2010
... www.ampcometal.com Ampcoloy is a registered trademark of Ampco Metal SA. Table 1 Mechanical properties Property Nominal values Ultimate tensile strength, MPa (ksi) 758 (110) Yield strength, RP 0.5, MPa (ksi) 386 (56) Elongation 2 in., % 16 Brinell hardness, HB 30 207 Rockwell hardness, HRB 95 Reduction of area, % 16...
Journal Articles
Alloy Digest (1982) 31 (9): Cu-444.
Published: 01 September 1982
... castability chemical composition corrosion-resistant alloys elasticity fatigue resistance hardness heat treatability joinability machinability marine hardware physical properties tensile properties wear resistance UNS C95500 1 Filing Code: CU-444 AMPCO D4 Copper Alloy Oir SEPTEMBER 1982 BIGlsT...
Journal Articles
Alloy Digest (1994) 43 (1): Cu-595.
Published: 01 January 1994
...) 59(407MPa) Elongation, % in 2 (5 1 mm) 25 23 Reduction of area, % 22 22 BHN (3000 kg.) l/4 (6.4 mm) deposit 187 1% PROPERTiES General Characteristics: AMPCO-TRODE 46 nickel-aluminum bronze spooled wire, barn md and czoated elect&es were developed for the welding of cast and wrought nickel-aluminum...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-580.
Published: 01 January 1993
... AMPCO-TRODE 7 is an iron-free aluminum bronze alloy available for overlay welding, particularly surfaces requiring a 125 BHN for wear while being able to resist corrosion from salts and sea water. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... AMPCO-TRODE 182 is a chromium-copper alloy filler metal that has high conductivity with good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-589. Producer...
Journal Articles
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... is rated 120% (same feed and depths). This analogy is valid for conventional machine-tools, as well as for CNC and high speed machining (HSC) centers. See Table 1 for comparisons. Table 1 Ampco alloys compared in hardness and cutting speed Material Brinell hardness, HB 30/10 Cutting speed, % 1.7225 (DIN 42...
Journal Articles
Alloy Digest (1978) 27 (4): Cu-352.
Published: 01 April 1978
... test-bar values or 1 -inch rounds where applicable. **Under load. 95000 50000 18 Heat Treatment: Ampco 483 can be hardened or strengthened by thermal treatment. Castings are used in the as-cast or temper- annealed condition. Wrought material can be hardened and strengthened by cold working...
Journal Articles
Alloy Digest (1955) 4 (5): Cu-26.
Published: 01 May 1955
... service on soft steel shafts as it seats i&f, char is, adjusts itself ro peculiarities of the shaft more quickly and easily than the harder, tougher grades of alumimm bronze. Specification Equivalents: Federal QCJ-B671b, CIass 1, Type I Ampco MetaI 12 retains a gwd proportion of its strength...
Journal Articles
Alloy Digest (1960) 9 (10): Cu-93.
Published: 01 October 1960
... Ampco Metal 21 is an aluminum bronze having high hardness, good compressive strength and resistance to wear and corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1993) 42 (6): Cu-584.
Published: 01 June 1993
... FOR DISSIMILAR WELDING- For determining the maximum Interpass and Preheat Temperature for various alloy R c G c A R A c - CA- STFFL R l-l G D C n n 0 - CAST IRON CCGCBCCC A=1 50°F (66%) maximum: B=300°F (149°C): C=4OO F (204°C); D=500 F (260°C): G=lOOO F (538°C) General Characteristics: AMPCO-TRODE 160...
Journal Articles
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
... of AMPCO Metal, Inc. Composition, Wt. %: Coated Electrodes Bare Wire (deposited weld metal) (filler metal) CoppeP Balance Balance Aluminum 14.0-15.0 14.0-15.0 Iron 3.0-5.0 3.0-5.0 Silicon 1.0 max. 0.04 max. OthlXS 0.50 max. 0.50 max. *Including Silver Table 1 - TYPICAL MECHANICAL PROPERTIES (Nominal all...
Journal Articles
Alloy Digest (1958) 7 (6): Cu-64.
Published: 01 June 1958
... strength chemical composition compressive strength corrosion-resistant alloys elasticity fatigue properties fracture toughness hardness joinability machinability physical properties shear strength tensile properties wear resistance workability - h 1 Filing Code: Cu-64 1 AMPCO 15 Copper...
Journal Articles
Alloy Digest (1961) 10 (9): Cu-107.
Published: 01 September 1961
... AMPCO 22 is a hard, low ductility aluminum bronze recommended for drawing and forming dies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1957) 6 (6): Cu-51.
Published: 01 June 1957
... AMPCO METAL 18 is an alpha-beta aluminum bronze having high resistance to wear and fatigue. It has high strength combined with good ductility and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (1980) 29 (1): Cu-388.
Published: 01 January 1980
... AMPCO 495 is a copper-aluminum-manganese-iron-nickel alloy characterized by high hardness and strength, excellent resistance to corrosion and good resistance to fatigue and wear. It is suited for service up to 700 F. Its many uses include bushings, valves, marine hardware and safety tools...
Journal Articles
Alloy Digest (1955) 4 (2): Cu-23.
Published: 01 February 1955
... AMPCO METAL-8 is a wrought alpha phase aluminum bronze possessing high tensile, impact and faigue characteristics. It is non-magnetic and resistant to sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1993) 42 (2): Cu-582.
Published: 01 February 1993
... A5.7 Class ER CuAL42 DOI: 10.31399/asm.ad.cu0582 Copyright © ASM International® 1996 Table 4 -MACHINING AMPCO-TRODE 10 TOOL DATA -SPEEDS AND FEEDS (Conventional Equipment with standard motors) CARBIDE INSERT CEMENTED CARBIDE SLIGHTLY POSTNE HONED EOOE GRIN-D 1 SIDE OF WEB l/32- ALL DRILLS MUST HAVE...