... AMPCO 483 is a copper-base alloy that can be used in the cast or wrought form. It provides high strength, high hardness, excellent resistance to corrosion and good resistance to fatigue and wear. It is well suited for service at temperatures up to 750 F and for applications such as pickling...
Journal Articles
Alloy Digest (1994) 43 (1): Cu-595.
Published: 01 January 1994
... (4.0mm); and 1 l/2 lb spools (68Kg) in -035 (0.8mm) and 0.045 (1.2mm) Applications: Ship fittings, Ship propellers, power plant valves, piping systems, intake screens, welding AMPCO 483, welding AMPCO 45, welding AMPCO D4, marine propulsion systems, propeller gear housing, oil recovery pumps. Producer...