Alloy Digest (1999) 48 (5): Ni-551.
Published: 01 May 1999
...: AMETEK Specialty Metal Products. Producer or Source: AMETEK Specialty Metal Products Copyright ┬ę ASM International┬« 1999 1999 ASM International AMETEK 899 NICKEL chemical composition hardness microstructure physical properties tensile properties thermal properties UNS N02270 N02201...