Alloy Digest (1999) 48 (6): CS-132.
Published: 01 June 1999
... composition, physical properties, and tensile properties. Filing Code: CS-132. Producer or source: American Alloy Steel Inc. Producer or Source: American Alloy Steel Inc. Copyright Ā© ASM InternationalĀ® 1999 1999 ASM International AMERICAN ALLOY TUF-37 chemical composition physical properties...