Alloy Digest (1974) 23 (2): Ni-200.
Published: 01 February 1974
... AMDRY 761 is a nickel-base alloy designed to provide maximum resistance to combinations of abrasion, corrosion, heat and oxidation. It is deposited by spraying on the desired surface at a thickness usually limited to a maximum of 0.080 inch. The data pertain to the deposit after fusing...
Journal Articles
Alloy Digest (1974) 23 (3): Ni-202.
Published: 01 March 1974
... usage as AMDRY 761 but thicker deposits can be made. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as heat...
Journal Articles
Alloy Digest (1974) 23 (10): Ni-209.
Published: 01 October 1974
... AMDRY 756 is a nickel-base alloy formulated to provide excellent resistance to combinations of abrasion, corrosion, heat and oxidation, and with better machinability characteristics than AMDRY 761. It is deposited by spraying on the desired surface at a thickness usually limited to a maximum...