Alloy Digest (1974) 23 (4): Ni-204.
Published: 01 April 1974
... AMDRY 755 is a nickel-base alloy designed to provide good resistance to combinations of abrasion, corrosion, impact, heat and oxidation. The alloy has good machinability characteristics and is easier to machine than AMDRY 756. It is deposited by spraying on the desired surface at a thickness...