Alloy Digest (1974) 23 (1): Ni-199.
Published: 01 January 1974
... AMDRY 754 is a nickel-base alloy formulated to provide good resistance to combinations of abrasion, corrosion, heat, impact shock and oxidation. It is deposited by spraying on the desired surface at a thickness usually limited to a maximum of 0.080 inch. Properties are on the deposit...