Alloy Digest (1953) 2 (2): Cu-5.
Published: 01 February 1953
... AMBRALOY 917 is a heat treatable aluminum bronze combining high strength with excellent resistance to corrosion. It is wear and abrasion resistant. It is also nonmagnetic and resistant to sparking. This datasheet provides information on composition, physical properties, hardness, and tensile...