Alloy Digest (1991) 40 (3): Al-313.
Published: 01 March 1991
... ALUMINUM ALLOY 390 is an aluminum die casting alloy with a controlled copper content of 4.0-5.0%. It is the most notable hypereutectic alloy of the aluminum-silicon series. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1971) 20 (8): Al-203.
Published: 01 August 1971
... REYNOLDS 390 and A390 are hypereutectic aluminum-silicon alloys having excellent wear resistance coupled with good mechanical properties, high hardness, and low coefficients of expansion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
... International Brush Alloy 390 chemical composition deformation properties elasticity fatigue properties fracture toughness high-temperature alloys physical properties thermal conductivity UNS C17460 Chemical Composition, wt Nickel 1.0 1.4 Beryllium 0.15 0.50 Aluminum 0.20 max Iron 0.20 max...
Journal Articles
Alloy Digest (2004) 53 (6): Al-390.
Published: 01 June 2004
... machines, housings and frames for food machinery, and base plates for high-voltage insu- lators. GIANTAL Filing Code: Al-390 Aluminum June 2004 GIANTAL (Aluminum Mold Alloy) Giantal is a wrought aluminum alloy for mold applications such as low-pressure plastic and composite molding, including thermoforming...
Journal Articles
Alloy Digest (2020) 69 (5): Al-464.
Published: 01 May 2020
... Raffmetal EN AB-Al Cu4Ti is a heat-treatable, aluminum-copper-titanium casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring high strength at temperatures up to 200 °C (390 °F). This alloy’s outstanding...
Journal Articles
Alloy Digest (1955) 4 (4): Al-25.
Published: 01 April 1955
... ALUMINUM 4032, formerly known as Aluminium 32S, is a forging alloy having comparatively low coefficient of expansion and good forgeability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1985) 34 (6): Al-258.
Published: 01 June 1985
... ALUMINUM A356.0 is a sand and permanent-mold casting alloy. It responds to an age-hardening heat treatment. This alloy has a relatively good combination of strength and ductility in the solution-treated and aged condition. Aluminum A356.0 is recommended for aircraft and missile components where...
Journal Articles
Alloy Digest (1985) 34 (9): Al-260.
Published: 01 September 1985
... ALUMINUM 707.0 is an aluminum-base foundry alloy that can be hardened by aging at room temperature without a solution treatment. It offers good strength in the cast-and-aged condition. It has relatively good castability, excellent machinability and high resistance to corrosion. Its many uses...
Journal Articles
Alloy Digest (1976) 25 (5): Al-223.
Published: 01 May 1976
... ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings and...
Journal Articles
Alloy Digest (2020) 69 (3): Al-462.
Published: 01 March 2020
... Raffmetal EN AB-Al Cu4MgTi is a heat-treatable, aluminum-copper-magnesium-titanium casting alloy in ingot form for remelting. It is used for producing sand, permanent mold, and investment castings for applications requiring high strength at temperatures up to 200 °C (390 °F). This alloy’s...
Journal Articles
Alloy Digest (1995) 44 (6): Al-335.
Published: 01 June 1995
.../asm.ad.al0335 Copyright © ASM International® 1996 Heat Treatment: See Table 2. For I7 Temper, 390°F (2oooC), hold at temperature 8h For T6 Temper, 3 lOoF (155 C). hold at temperature 8h For T4 Temper, room temperature General Characteristics: Aluminum alloy 206.0 and A2O6.0 have the nominal com- position range...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (1988) 37 (10): Cu-542.
Published: 01 October 1988
... ranks among the best acid resisting high-strength alloys. Specification Equivalents:* UNS CY5400 ASTM B505(C95400), B148(954) Federal -390 Alloy C95400 Type III *Replace previously used common trade name specifications. General Characteristics: Continuous Cast Aluminum Bronze. resists deformation under...
Journal Articles
Alloy Digest (1953) 2 (5): Al-7.
Published: 01 May 1953
... 660-720.F. hold at tunpratnre for 24 Nz: kTHat to 960-98O F bold at mnpaann 2 hours, air owl r&at to 390-F for 2 hours, air COOL (rititholding Workabiiityz Good fomabihy. For kot forging ptthat at 970°F, and forge in raag of 970 to 900.F. down to 660-F. All cold working should be done in the znnepled...
Journal Articles
Alloy Digest (1957) 6 (11): Al-59.
Published: 01 November 1957
... TERNALLOY 6 is an age-hardenable aluminum alloy having good castability, excellent machinability, and high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat...
Journal Articles
Alloy Digest (1959) 8 (11): Al-86.
Published: 01 November 1959
... RED X-11 is a heat treatable aluminum alloy of the silicon-copper-magnesium type. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as...
Journal Articles
Alloy Digest (1978) 27 (8): Cu-359.
Published: 01 August 1978
... Copper Alloy No. 955 is a copper-aluminum-iron-nickel alloy with high strength and hardness, good resistance to fatigue and wear, and excellent resistance to corrosion. It is suited for service up to 750 F. Typical applications are marine hardware, gears and pickling equipment. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (6): Cu-397.
Published: 01 June 1980
... Copper Alloy No. C95800 is a copper-aluminum-nickel-iron-manganese alloy with high strength and hardness. It also is characterized by excellent resistance to corrosion and good resistance to fatigue and wear. It is suited for service up to 750 F. Typical uses comprise hubs and blades of ship...
Journal Articles
Alloy Digest (1977) 26 (2): Cu-326.
Published: 01 February 1977
.... Specification Equivalents: ASTM B 148 (Aluminum bronze 952, formerly desig- nated 9A). UNS No. C95200. Ingot No. 415. ASTM: B 30, B 271 and B 505. Federal: QQ-C-390. Military: MIL-C-22229, Composition 5. SAE: J461 and 3462. General Characteristics: Copper Alloy No. 952 is a cast aluminum bronze containing...
Journal Articles
Alloy Digest (2005) 54 (4): Cu-733.
Published: 01 April 2005
... MoldStar 18 has good bearing qualities and has resistance to wear, abrasion, fatigue, deformation, and corrosion. MoldStar 21 and 22 are harder alloys and also have good bearing qualities and resistance to wear, abrasion, fatigue, deformation, and corrosion. This family of aluminum bronzes is used...