Alloy Digest (1973) 22 (2): Al-179.
Published: 01 February 1973
... ALUMINUM 7075 is a wrought precipitation-hardenable aluminum alloy having excellent mechanical properties, workability and response to heat treatment and refrigeration. (This alloy is covered under its previous designation, ALUMINUM 75S, in Alloy Digest Al-5, February 1953). This datasheet...
Journal Articles
Alloy Digest (2000) 49 (3): Al-368.
Published: 01 March 2000
... Kaiser Aluminum Alloy 7075 has high mechanical properties and, in the T73 and T74 tempers, offers improved corrosion-cracking resistance. The alloy has good machinability. It is typically used in aircraft structural parts. (See also Alloy Digest Al-457, January 2019.) This datasheet provides...
Journal Articles
Alloy Digest (1990) 39 (11): Al-309.
Published: 01 November 1990
... AA 7075 is the outstanding alloy of the 7000 series heat-treatable wrought aluminum alloys. It is used for highly stressed parts. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength. It also includes information on low...
Journal Articles
Alloy Digest (1986) 35 (7): Al-269.
Published: 01 July 1986
... tempers are immune to stress-corroston cracking. The T76 type tempers are exiolia:ion resistant and hn\*e good resistance to stress-corroston cracking. Specification Equivalents: Aluminum 7075 A 7075). .ASTM B 209. B 210. B ?I I. B 221. B 241. B 247 and B 316. AhZS: 4044. 4045. 4078. 412 . 4123. 4124...
Journal Articles
Alloy Digest (1962) 11 (7): Al-116.
Published: 01 July 1962
... corrosion when heat treated and fully aged. Specification Equivalents: Brit. D.T.D. 5064 Aluminum 7075 (nearest U.S. Spec.) Impalco 760 responds to a precipitation hard- ening heat treatment to produce rhe highest mechanical properties. However, it exhibits a high degree of notch sensitivity. Forms...
Journal Articles
Alloy Digest (1989) 38 (4): Al-295.
Published: 01 April 1989
... IncoMAP alloy A1-905XL is a low density aluminum alloy designed to replace alloy 7075-T73 in forgings where weight is critical. Its density is 8% less than that of alloy 7075-T73. Heat treatment is not required to develop its strength. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
.... AMS 4228fl6), AMS 4229(T7) and AhfS 4223(T43). General Characteristics: Aluminum A201 is an aluminum-base casting alloy that exhibits exceptionally high strength. It is the strongest aluminum casting alloy commercially available today. Furthermore, it rivals the strength of Aluminum 7075-T73 forgings...
Journal Articles
Alloy Digest (1963) 12 (4): Al-124.
Published: 01 April 1963
... and artificial aging. Its re- sistance to atmospheric attack is poor. It is un- suitable for brightening and anodizing. Specification Equivalents: Brit. D.T.D. 5044 Brit. D.T.D. 5024 Aluminum 7075 (Nearest U.S. Spec.) General Characteristics: Impalco 740 responds to an age hardening heat treatment to produce...
Journal Articles
Alloy Digest (1989) 38 (9): Al-299.
Published: 01 September 1989
... ALCOA Alloy 2090 is an aluminum-lithium alloy with 8% lower density and 12% higher elastic modulus than 7075-T6, a major high-strength alloy used in aircarft structures. Special facilities and practices required for casting commercial size aluminum-lithium ingots have been developed to cope...
Journal Articles
Alloy Digest (2008) 57 (6): Al-414.
Published: 01 June 2008
... Kaiser Aluminum alloy 7175/7475 is a high-purity version of 7075 and is heavily used by the aircraft and ordinance industries because of its superior strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1963) 12 (1): Al-22.
Published: 01 January 1963
... of Aluminum 7075. ALUMINUM 7001 responds to an age-hardening heat treatment to produce the highest mechanical properties of all the aluminum alIoys. However, it exhibits a high degree of notch sensitivity. In working this alloy in the solution treated condition, it strain-hardens more rapidly than the 24s.W...
Journal Articles
Alloy Digest (1999) 48 (12): Al-364.
Published: 01 December 1999
... Finkl Alu-C is a modification of UNS A92618 with higher thermal conductivity and higher yield strength above 121 C (250 F) than aluminum alloy 7075-T651. Alu-C is used for general, low-volume plastic injection molds. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2005) 54 (9): Al-397.
Published: 01 September 2005
... Alloy 7055 extruded products in the T74511 and T76511 tempers have a combination of high strength, excellent corrosion resistance, toughness, fatigue, and formability. The alloy was developed as an advance over aluminum alloys 7178 and 7075. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2019) 68 (1): Al-457.
Published: 01 January 2019
... of thermal expansion, 10 6/K (10 6/°F) Linear, 20 100 °C (68 212 °F) 23.4 (13.0) Volumetric, 20 °C (68 °F) 6.80 (3.78) Copyright © 2019, ASM International®. All rights reserved. KAISER ALLOY 7075 (High-Strength Alloy) Filing Code: Al-457 Aluminum :: January 2019 Materials Park, Ohio 44073-0002...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
... International ALCOA 7075 chemical composition corrosion-resistant alloys machinability physical properties tensile properties wrought aluminum alloys thermal properties - DIGEST - DATA ON WORLD WiDE METALS AND ALLOYS pydght 7996, ASM htematiwnl. At/ nghts resawed.Datashownaretypica/.nottoba used...
Journal Articles
Alloy Digest (2004) 53 (5): Al-388.
Published: 01 May 2004
... is the highest-strength aluminum plate alloy/temper currently available for commercial aircraft applications. A controlled toughness alloy with guaranteed levels of fracture toughness; this alloy is a potential replacement for 7075-T651 since it provides 41.4 68.9 MPa (6 10 ksi) higher strength levels. Alloy...
Journal Articles
Alloy Digest (1959) 8 (10): Al-84.
Published: 01 October 1959
... and notched speci- mens, in longitudinal and transverse directions. This alloy is at least equal to and probably superior to 7075-T6 from the standpoint of suess-corrosion aack- ing in salr water atmospheres. Aluminum 7079 responds well to an age-hardening heat treatment for maximum strength and hardness...
Journal Articles
Alloy Digest (1990) 39 (5): Cp-15.
Published: 01 May 1990
... resistance powder metal products SXA tensile properties - DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS SXA@ Filing Code: Composite cp15 MAY 1990 P&t&bed& Alby Digest hc.1201-677-6161 27 Canfii Slmet, Orange, NJ. 07650 I USA SXA= (Discontinuously Reinforced Aluminum Alloys) SXA@ is a unique group...
Journal Articles
Alloy Digest (2017) 66 (1): Al-450.
Published: 01 January 2017
... 2.4 3.0 Lithium 1.6 2.0 Zirconium 0.05 0.12 Iron 0.07 max Silicon 0.05 max Titanium 0.10 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Mechanical Properties: Mechanical properties are shown in Table 1 while fracture toughness is in Table 2. S-N fatigue is in Fig. 1, and FCG curves...
Journal Articles
Alloy Digest (2000) 49 (7): Al-371.
Published: 01 July 2000
... Zinc 0.10 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3) 2590 (0.093) Mechanical Properties: See Table 1. Weldability: The welding response of 2090-T83 sheet is superior to that of 2024-T3 and 7075-T6 sheet. Corrosion Resistance: Long-term...