Alloy Digest (1985) 34 (9): Al-260.
Published: 01 September 1985
... ALUMINUM 707.0 is an aluminum-base foundry alloy that can be hardened by aging at room temperature without a solution treatment. It offers good strength in the cast-and-aged condition. It has relatively good castability, excellent machinability and high resistance to corrosion. Its many uses...
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... Malleable iron Aluminum Alloy 208.0 Temalloy 7 Cutting speed, surface ft min 250 275 II00 5ooo APEX TERNALLOY 7 retains its white coloring where it is exposed to weathering. It is more resistant to corrosion than other aluminum alloys. Specification Equivalents: AA 707.0. ASTM:B 2q707.0) and B 108(707.0...