1-17 of 17 Search Results for

ALUMINUM 6262

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1980) 29 (12): Al-182.
Published: 01 December 1980
... ALUMINUM 6262 is an alloy with an excellent combination of machinability, strength and resistance to corrosion. Lead and bismuth are added to provide free-machining characteristics. Its many applications include screw-machine products, housewares, marine parts. aerospace fittings and general...
Journal Articles
Alloy Digest (1999) 48 (9): Al-361.
Published: 01 September 1999
... Kaiser Aluminum alloy 6262 (Tennalum alloy 6262) is an Al-Mg-Si-Cu-Cr-Pb-Bi alloy with characteristic good machinability and corrosion resistance and a good acceptance of coatings (anodize response). It is typically used in automotive parts, fittings, building hardware, and valve components...
Journal Articles
Alloy Digest (1999) 48 (10): Al-362.
Published: 01 October 1999
... Kaiser Aluminum alloy KA62 (Tennalum alloy KA62) is a lead-free alternative to 6262. It offers good machinability and corrosion resistance and displays good acceptance of coatings (anodize response). It can be used in place of 6262 because its physical and mechanical properties are equivalent...
Journal Articles
Alloy Digest (1996) 45 (12): Al-340.
Published: 01 December 1996
... UltrAlloy is a lead-free, enhanced machining product with the inherent benefits of a 6xxx-series alloy. The alloy is produced as a cold-finished rod and bar with strength levels comparable to 6262. The alloy is registered with the Aluminum Association as X6020. This datasheet provides information...
Journal Articles
Alloy Digest (2010) 59 (10): Al-432.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum October 2010 Al-432 Kaiser Alloy 6041 is a lead-free alternative to 6262 with good corrosion resistance. KAISER ALLOY 6041 (Extruded Rod & Bar) KAISER ALLOY 6041 Chemical Composition, wt (Nominal) Silicon 0.50...
Journal Articles
Alloy Digest (2016) 65 (11): Al-448.
Published: 01 November 2016
... to replace or substitute for alloy 6262. Producer: Kaiser Aluminum Corporation Foothill Ranch, CA 92610, USA Tel: (949) 614-1740 www.kaiseraluminum.com ISSN: 002-614X Al-448B ...
Journal Articles
Alloy Digest (2016) 65 (12): Al-449.
Published: 01 December 2016
... or substitute for alloy 6262. Producer: Kaiser Aluminum Corporation Foothill Ranch, CA 92610, USA Tel: (949) 614-1740 www.kaiseraluminum.com ISSN: 002-614X Al-449B ...
Journal Articles
Alloy Digest (1998) 47 (8): Al-351.
Published: 01 August 1998
... design. Filing Code: Al-351 i?El Aluminum u - August 1998 Pubtkhed ty ASM tntemabonat Materials Park, Ohio 4407LWlX32 440-J38-5151 Fax440-3384634 Mem-Senrepo.ASM-lntl.org ALCOA 6262 (Machinable High-Strength Alloy) Alcoa 6262 ahoy has good machinability with high strength, high corrosion resistance...
Journal Articles
Alloy Digest (1998) 47 (9): Al-353.
Published: 01 September 1998
... Alcoa C238 is a cold-finished aluminum wrought product developed for applications requiring postbrazing and welding strength. The alloy has good machinability and roll-threading characteristics. It has slightly lower corrosion resistance as compared to 6xxx series alloys. Alloy C238 has excellent...
Journal Articles
Alloy Digest (1998) 47 (5): Al-348.
Published: 01 May 1998
... Alcoa Excalibar 6013 alloy has high strength, good machinability, and good corrosion resistance. It is easily joined by all welding and brazing methods, has excellent compressive properties, and has good applied coating acceptance. See also Alcoa Aluminum Alloy 6013, Alloy Digest Al-282, revised...
Journal Articles
Alloy Digest (2008) 57 (3): Al-411.
Published: 01 March 2008
... Kaiser Aluminum Alloy 6040 has good strength and good corrosion resistance. It was developed for machinability with low lead content. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2006) 55 (12): CS-147.
Published: 01 December 2006
... automotive industry chemical composition construction materials fatigue properties physical properties TENFORM XF350 tensile properties workability Chemical Composition, wt (Typical Analysis) Carbon <0.10 Manganese <1.20 Silicon <0.04 Phosphorus <0.025 Sulfur <0.01 Aluminum <0.02 Niobium <0.3 Iron...
Journal Articles
Alloy Digest (2007) 56 (1): CS-148.
Published: 01 January 2007
... 0.01 Aluminum 0.02 Niobium 0.3 Iron bal Physical Properties: (Typical) Density, kg/m3 (lb/in.3) 7800 (0.28) Mechanical Properties: (Test pieces taken in the rolling direction) Yield strength, MPa (ksi) Typical 450 (65) 2 3 mm thick 486 (70) Tensile strength, MPa (ksi) Typical 500 (73) 2 3 mm thick...
Journal Articles
Alloy Digest (1998) 47 (4): Al-347.
Published: 01 April 1998
...&338-4634 Mm-ServOpo.ASA.4~lntkq DELTALLOY 4032@ (Wear and Abrasion Resistant Alloy) Filing Code: Al-347 a Aluminum u - April 1998 Deltalloy 4032 has good machinability and drilling characteristics when using single-point or multispindle screw machines and an excellent surface finish using...
Journal Articles
Alloy Digest (2000) 49 (2): Ni-558.
Published: 01 February 2000
..., and 230-W is a trademark of Haynes International, Inc. Chemical Composition, wt (Nominal) Nickel 57 (as balance) Cobalt 5 max Chromium 22 Molybdenum 2 Tungsten 14 Iron 3 max Silicon 0.4 Manganese 0.5 Carbon 0.07 Aluminum 0.3 Boron 0.002 max Physical Properties: Density, kg/m3 (lb/in.3) 8830 (0.319...
Journal Articles
Alloy Digest (2012) 61 (11): CS-173.
Published: 01 November 2012
... Manganese 1.50 Silicon 0.35 Phosphorus 0.025 Sulfur 0.01 Aluminum 0.02 Niobium 0.3 Iron bal Physical Properties: (Typical) Density, kg/m3 (lb/in.3) 7800 (0.28) Mechanical Properties: High strain rate properties are shown in Table 1; typical properties are in Table 2. Fatigue values are shown...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity...