Alloy Digest (1978) 27 (4): Al-121.
Published: 01 April 1978
... ALUMINUM 5457 is an aluminum sheet alloy that offers a lustrous, mirror-like appearance when polished, brightened and anodized. The brightness of the specially treated sheet makes it particularly desirable for decorative trim applications in the appliance and automotive industries. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (8): Al-178.
Published: 01 August 1980
... radii are given in Table 3. Its cold-forming characteristics are similar to those of Aluminum 3003 and Aluminum 5457. Joinability: Aluminum 5657 is generally weldable by all commercial procedures and methods, particularly by the gas, arc and resistance spot and seam methods. Frequently used fiUer metals...
Journal Articles
Alloy Digest (1991) 40 (6): Al-317.
Published: 01 June 1991
... AA 5657 is a binary aluminum/magnesium alloy of moderate strength. It is not hardenable by heat treatment. It is strain hardenable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information...
Journal Articles
Alloy Digest (1968) 17 (6): Al-176.
Published: 01 June 1968
... Aluminum 5557 is an aluminum alloy having good bright finishing characteristics. It has good formability and weldability. It is recommended for finishing and decorative applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...